Comparison of Magnetic Properties of Low-Temperature-Fired NiCuZn Ferrites Under Low- and High-Bi2O3 Doping Modes

被引:0
作者
Yang Wang
Yulan Jing
Shenglei Che
Yuanxun Li
Zhiqiang Xu
Xiaoli Tang
机构
[1] University of Electronic Science and Technology of China,State Key Laboratory of Electronic Thin Films and Integrated Devices
[2] Zhejiang University of Technology,College of Materials Science and Engineering
来源
Journal of Electronic Materials | 2020年 / 49卷
关键词
NiCuZn ferrite; permeability; microstructure; Q-factor; DC-bias-superposition;
D O I
暂无
中图分类号
学科分类号
摘要
Phase composition, microstructure and magnetic properties of the low-temperature-fired NiCuZn ferrites doped with different concentrations of Bi2O3 were investigated. A proper content of Bi2O3 doping could trigger the formation of a dual microstructure of the ferrites. The before and after ‘critical’ doping content, i.e. low- and high-Bi2O3-doping modes,enabled the ferrites to obtain sufficiently high density and equal permeability. The former sample obtained a uniform, dense and fine-grain-sized microstructure, which was beneficial to improve the high-frequency characteristic and Q-factor characteristic of the low-temperature-fired NiCuZn ferrite; moreover, the saturation flux density was higher. However, the latter sample obtained a uniform, dense and large-grain-sized microstructure with more grain-boundary-dopant, which was beneficial to improve the DC-bias superposition characteristic of the ferrite. These comparative results can essentially guide the engineering applications of the low-temperature-fired NiCuZn ferrites.
引用
收藏
页码:3325 / 3331
页数:6
相关论文
共 130 条
  • [1] Zhu J(2016)undefined J. Magn. Magn. Mater. 407 308-undefined
  • [2] Ouyang C(2018)undefined Ceram. Int. 44 2304-undefined
  • [3] Xiao S(2013)undefined Ceram. Int. 39 3077-undefined
  • [4] Gao Y(2014)undefined J. Alloys Compd. 595 206-undefined
  • [5] Hua S(2004)undefined J. Magn. Magn. Mater. 283 157-undefined
  • [6] Zhao C(2014)undefined J. Electron. Mater. 43 299-undefined
  • [7] Guo H(1999)undefined J. Am. Ceram. Soc. 82 343-undefined
  • [8] Wang Q(2015)undefined J. Magn. Magn. Mater. 374 367-undefined
  • [9] Dai C(2012)undefined J. Magn. Magn. Mater. 324 578-undefined
  • [10] Zhang H(2016)undefined J. Alloys Compd. 660 398-undefined