摘要
To obtain a better understanding of the mechanical properties and failure characteristics of the single-crystal Fe-3%Al alloy (SC), tensile and fatigue properties of the SC and polycrystalline Fe-3%Al alloy (PC) have been investigated. The tensile strength and fracture strain for the SC samples were different depending on the loading direction, i.e., 〈111〉, 〈110〉 and 〈100〉, which could be explained by the Schmid factor. Fatigue strength for the SC samples was basically correlated with their tensile strength. Different fatigue properties were obtained for the PC sample, e.g., the high fatigue strength was obtained in the early fatigue stage, and significant reduction in the fatigue strength was appeared in the later fatigue stage, e.g., low endurance limit at 107 cycles. The reason for this was caused by the material brittleness due to the accumulated dislocation at the grain boundaries. Because the high ductile SC samples made severe plastic deformation ahead of the crack tip, the crack growth rate did not enhance even if the high stress intensity factor range was applied in Region II (da/dN versus ΔK). The crack growth rate dropped just before the final fracture. Effective stress intensity factor range was estimated using the crack closure model, but the crack growth rate is found to be affected strongly by the slip system of SC sample.
引用
收藏
页码:5978 / 5987
页数:9
相关论文
共 50 条
  • [21] Parameters influencing the fatigue life of a Cu-Al-Be single-crystal shape memory alloy under repeated bending
    Siredey-Schwaller, N.
    Eberhardt, A.
    Bastie, P.
    SMART MATERIALS & STRUCTURES, 2009, 18 (02):
  • [22] Development of Cell Structure and Crack Initiation during Fatigue of an Fe-3 mass%Si Alloy
    Nakano, Hirotaka
    Miyazawa, Tomotaka
    Shuto, Hiroshi
    Fujii, Toshiyuki
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2023, 109 (01): : 76 - 85
  • [23] Thermal cycle fatigue behaviors of a single crystal Ni3Al base alloy
    Li, Fulin
    Li, Shusuo
    Wu, Yuxiao
    Jiang, Liwu
    Han, Yafang
    2011 CHINESE MATERIALS CONFERENCE, 2012, 27 : 1141 - 1149
  • [24] Influence of copper on the deformation and primary recrystallization of Fe-3% Si alloy single crystals
    A. A. Redikul’tsev
    A. S. Yurovskikh
    Redikul'tsev, A. A., 1600, Allerton Press Inc, 18 West 27th Street, New York, NY 10001, United States (42): : 399 - 404
  • [25] Special misorientations in localized deformation regions in Fe-3%Si alloy single crystals
    Rusakov, G. M.
    Lobanov, M. L.
    Redikul'tsev, A. A.
    Karabanalov, M. S.
    Lobanova, L. V.
    TECHNICAL PHYSICS, 2014, 59 (08) : 1180 - 1184
  • [26] LAPPING CHARACTERISTICS OF LINBO3 SINGLE-CRYSTAL
    NODA, J
    IDA, I
    REVIEW OF THE ELECTRICAL COMMUNICATIONS LABORATORIES, 1972, 20 (1-2): : 152 - &
  • [27] Special misorientations in localized deformation regions in Fe-3%Si alloy single crystals
    G. M. Rusakov
    M. L. Lobanov
    A. A. Redikul’tsev
    M. S. Karabanalov
    L. V. Lobanova
    Technical Physics, 2014, 59 : 1180 - 1184
  • [28] MICROSCOPY AND MICROINDENTATION MECHANICS OF SINGLE-CRYSTAL FE-3 WT-PERCENT-SI .2. TEM OF THE INDENTATION PLASTIC ZONE
    ZIELINSKI, W
    HUANG, H
    GERBERICH, WW
    JOURNAL OF MATERIALS RESEARCH, 1993, 8 (06) : 1300 - 1310
  • [29] Decarburizing annealing of technical alloy Fe-3% Si
    Lobanov, ML
    Gomzikov, AI
    Akulov, SV
    Pyatygin, AI
    METAL SCIENCE AND HEAT TREATMENT, 2005, 47 (9-10) : 478 - 483
  • [30] Secondary recrystallization of the nitrided Fe-3%Si alloy
    Woo, JS
    Han, CH
    Hong, BD
    Harase, J
    ISIJ INTERNATIONAL, 1998, 38 (10) : 1114 - 1120