Fatigue Failure Characteristics of Single-Crystal Fe-3%Al Alloy

被引:0
|
作者
Mitsuhiro Okayasu
Keisuke Noda
机构
[1] Okayama University,Graduate School of Natural Science and Technology
来源
Journal of Materials Engineering and Performance | 2019年 / 28卷
关键词
crack growth; failure characteristic; fatigue property; single crystal; steel;
D O I
暂无
中图分类号
学科分类号
摘要
To obtain a better understanding of the mechanical properties and failure characteristics of the single-crystal Fe-3%Al alloy (SC), tensile and fatigue properties of the SC and polycrystalline Fe-3%Al alloy (PC) have been investigated. The tensile strength and fracture strain for the SC samples were different depending on the loading direction, i.e., 〈111〉, 〈110〉 and 〈100〉, which could be explained by the Schmid factor. Fatigue strength for the SC samples was basically correlated with their tensile strength. Different fatigue properties were obtained for the PC sample, e.g., the high fatigue strength was obtained in the early fatigue stage, and significant reduction in the fatigue strength was appeared in the later fatigue stage, e.g., low endurance limit at 107 cycles. The reason for this was caused by the material brittleness due to the accumulated dislocation at the grain boundaries. Because the high ductile SC samples made severe plastic deformation ahead of the crack tip, the crack growth rate did not enhance even if the high stress intensity factor range was applied in Region II (da/dN versus ΔK). The crack growth rate dropped just before the final fracture. Effective stress intensity factor range was estimated using the crack closure model, but the crack growth rate is found to be affected strongly by the slip system of SC sample.
引用
收藏
页码:5978 / 5987
页数:9
相关论文
共 50 条
  • [1] Fatigue Failure Characteristics of Single-Crystal Fe-3%Al Alloy
    Okayasu, Mitsuhiro
    Noda, Keisuke
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (10) : 5978 - 5987
  • [2] Cyclic Deformation Behavior and Evolution of Dislocation Structure in Fe-3 mass%Al Alloy with Bcc Single Crystal
    Sakurada, Eisaku
    Hiwatashi, Shunji
    Ushioda, Kohsaku
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2017, 103 (03): : 157 - 165
  • [3] Tensile Properties and Work-hardening Behavior of Fe-3%Al Single Crystal
    Takemoto, Yoshito
    Senuma, Takehide
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2012, 98 (06): : 216 - 222
  • [4] Effect of crystallographic orientation on fatigue crack growth of an Fe-3 mass%Si single crystal
    Mine, Y
    Moriya, T
    Ando, S
    Takashima, K
    Tonda, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1998, 62 (02) : 150 - 158
  • [5] Effects of overload on fatigue crack propagation of Fe-3% Si alloy
    Makabe, Chobin
    Sakihama, Hisashi
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 1993, 59 (564): : 1800 - 1805
  • [6] THERMOLUMINESCENT RESPONSE OF SINGLE-CRYSTAL AL2O3-FE
    AYPAR, A
    APPLIED RADIATION AND ISOTOPES, 1986, 37 (09) : 961 - 963
  • [7] New Fe−Co−Ni−Cu−Al−Ti Alloy for Single-Crystal Permanent Magnets
    I. V. Belyaev
    V. E. Bazhenov
    A. V. Moiseev
    A. V. Kireev
    The Physics of Metals and Metallography, 2016, 117 : 214 - 221
  • [8] Fe-Al alloy single-crystal thin film preparation for basic magnetic measurements
    Abe, Tatsuya
    Kawai, Tetsuroh
    Futamoto, Masaaki
    Ohtake, Mitsuru
    Inaba, Nobuyuki
    AIP ADVANCES, 2018, 8 (04):
  • [9] Nitriding of Fe-3% Si alloy
    Lobanov M.L.
    Steel in Translation, 2015, 45 (2) : 94 - 99
  • [10] Growth morphology of single-crystal grains obtained by directional crystallisation of an Al-Cu-Fe alloy
    Surowiec, Marian
    Bogdanowicz, Wlodzimierz
    Krawczyk, Jacek
    Formanek, Boleslaw
    Sozanska, Maria
    PHILOSOPHICAL MAGAZINE, 2011, 91 (19-21) : 2458 - 2465