High-Temperature Phases in the Fe–Mo–Cr–C System

被引:0
|
作者
T. A. Velikanova
A. M. Zaslavskii
M. V. Kindrachuk
机构
[1] National Academy of Sciences of Ukraine,Frantsevich Institute for Problems of Materials Science
[2] State Reserve Agency of Ukraine,Research Institute ‘Resurs’
[3] National Aviation University,undefined
来源
Powder Metallurgy and Metal Ceramics | 2023年 / 61卷
关键词
Fe; Mo; Cr; C system; high-temperature phase equilibria; manganese-like phases; linear thermal expansion coefficients;
D O I
暂无
中图分类号
学科分类号
摘要
Phase equilibria involving the stable high-temperature quaternary χFe,Cr,Mo,C phase were established in the Fe–Mo–Cr–C phase diagram. The arc-melted alloys were annealed at subsolidus temperatures for 52 h and then quenched in liquid gallium. The solidus temperature of the alloys was determined with the Pirani–Alterthum method. High-temperature X-ray diffractometry was employed to monitor the sequence of changes in the alloy phase composition from room temperature to the solidus temperature. The χ + η + α, χ + η, and χ + σ phase equilibria were directly observed at 973 K < T < 1373 K, 1273 K < T < 1530 K, and 1523 K < T < 1530 K, respectively, in the Fe52.5Mo23.5Cr18.7C5.3 (at.%) alloy. The χ + M23C6 + α and χ + σ phase equilibria were directly observed at 973 K ≤ T < 1523 K and 1473 K < T < 1525 K in the Fe55.5Mo11.8Cr28.2C4.5 (at.%) alloy. It was shown that the two-phase χ + σ equilibrium could be preceded by three-phase χ + η + σ equilibria or a single-phase χ Fe,Cr,Mo,C equilibrium region (for the Fe52.5Mo23.5Cr18.7C5.3 alloy in the 1523 K < T < 1530 K temperature range). The quaternary χ Fe,Cr,Mo,C phase was found in the (51.9–64.9) Fe, (5.4–23.5) Mo, (14.5–35.4) Cr, and (1–10.7) C at.% composition ranges. Primary crystallization regions of the σ Fe,Cr,Mo,C and αFe,Cr,Mo,C phases with solidus temperatures of approximately 1530 K (for the Fe52.5Mo23.5Cr18.7C5.3 alloy) and 1525 K (for the Fe55.5Mo11.8Cr28.2C4.5 alloy) were revealed. The linear thermal expansion coefficients for the χ Fe,Cr,Mo,C, η Fe,Cr,Mo,C, and αFe,Cr,Mo,C phases of different composition observed for different temperature ranges were determined.
引用
收藏
页码:613 / 624
页数:11
相关论文
共 50 条
  • [41] High-temperature sulfidation of Al- and Mo-modified 310 stainless steel
    Kai, W
    Leu, CT
    Chu, JP
    Lee, PY
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 625 - 632
  • [42] Computer Simulated Diffraction Patterns of Laves Fe2Mo and μ-Fe7Mo6 Phases
    沙维
    RareMetals, 1992, (02) : 145 - 146
  • [43] Chemical diffusion of Al, Cr, Fe, Ni in steel weldments in the temperature range of 500-1100°C
    Kucera, J
    Million, B
    Stránsky, K
    KOVOVE MATERIALY-METALLIC MATERIALS, 2003, 41 (05): : 325 - 334
  • [44] Effect of precipitations on the damping capacity of Fe-13Cr-2.5Mo alloy
    Hu, Xiaofeng
    Li, Xiuyan
    Zhang, Bo
    Rong, Lijian
    Li, Yiyi
    SECOND INTERNATIONAL CONFERENCE ON SMART MATERIALS AND NANOTECHNOLOGY IN ENGINEERING, 2009, 7493
  • [45] High-Temperature Erosion of HVOF Sprayed Cr3C2-NiCr Coating and Mild Steel for Boiler Tubes
    Guan-Jun Yang
    Chang-Jiu Li
    Shi-Jun Zhang
    Cheng-Xin Li
    Journal of Thermal Spray Technology, 2008, 17 : 782 - 787
  • [46] Influence of Mo addition on the solvus temperature of Ni2(Cr,Mo) phase in Ni2(CF,MO) alloys
    Pai, H. C.
    Sundararaman, M.
    Maji, B. C.
    Biswas, A.
    Krishnan, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 491 (1-2) : 159 - 164
  • [47] High-temperature tribological property of Fe-based amorphous alloy coating
    Xu, Jun-jie
    Kang, Jia-jie
    Yue, Wen
    Fu, Zhi-qiang
    Zhu, Li-na
    She, Ding-shun
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2021, 573
  • [48] Microstructure evolution of a Cr-Cr/Mo coated Zr alloys in inert gas and steam environment at high temperature
    Yang, Jianqiao
    Ding, Yining
    Zhao, Fen
    Shang, Lunlin
    Cui, Yanguang
    Wang, Shuzhong
    Yun, Di
    Xu, Donghai
    JOURNAL OF NUCLEAR MATERIALS, 2024, 589
  • [49] Improvement of the high temperature oxidation of 1.10Cr-0.25Mo steel at 850 °C by hot-dip Al coating
    Badaruddin, Mohammad
    Supriadi, Harnowo
    Erwin
    INTERNATIONAL CONFERENCE ON ADVANCES SCIENCE AND CONTEMPORARY ENGINEERING 2012, 2012, 50 : 640 - 648
  • [50] Influence of Ta/Zr minor-alloying on the high-temperature microstructural stability of cladding Fe-Cr-Al ferritic stainless steels
    Anjum, M. Wasim
    Wen, Donghui
    Wang, Qing
    Zhang, Ruiqian
    Dong, Chuang
    Liaw, Peter K.
    JOURNAL OF NUCLEAR MATERIALS, 2019, 522 : 19 - 31