High-Temperature Phases in the Fe–Mo–Cr–C System

被引:0
|
作者
T. A. Velikanova
A. M. Zaslavskii
M. V. Kindrachuk
机构
[1] National Academy of Sciences of Ukraine,Frantsevich Institute for Problems of Materials Science
[2] State Reserve Agency of Ukraine,Research Institute ‘Resurs’
[3] National Aviation University,undefined
来源
Powder Metallurgy and Metal Ceramics | 2023年 / 61卷
关键词
Fe; Mo; Cr; C system; high-temperature phase equilibria; manganese-like phases; linear thermal expansion coefficients;
D O I
暂无
中图分类号
学科分类号
摘要
Phase equilibria involving the stable high-temperature quaternary χFe,Cr,Mo,C phase were established in the Fe–Mo–Cr–C phase diagram. The arc-melted alloys were annealed at subsolidus temperatures for 52 h and then quenched in liquid gallium. The solidus temperature of the alloys was determined with the Pirani–Alterthum method. High-temperature X-ray diffractometry was employed to monitor the sequence of changes in the alloy phase composition from room temperature to the solidus temperature. The χ + η + α, χ + η, and χ + σ phase equilibria were directly observed at 973 K < T < 1373 K, 1273 K < T < 1530 K, and 1523 K < T < 1530 K, respectively, in the Fe52.5Mo23.5Cr18.7C5.3 (at.%) alloy. The χ + M23C6 + α and χ + σ phase equilibria were directly observed at 973 K ≤ T < 1523 K and 1473 K < T < 1525 K in the Fe55.5Mo11.8Cr28.2C4.5 (at.%) alloy. It was shown that the two-phase χ + σ equilibrium could be preceded by three-phase χ + η + σ equilibria or a single-phase χ Fe,Cr,Mo,C equilibrium region (for the Fe52.5Mo23.5Cr18.7C5.3 alloy in the 1523 K < T < 1530 K temperature range). The quaternary χ Fe,Cr,Mo,C phase was found in the (51.9–64.9) Fe, (5.4–23.5) Mo, (14.5–35.4) Cr, and (1–10.7) C at.% composition ranges. Primary crystallization regions of the σ Fe,Cr,Mo,C and αFe,Cr,Mo,C phases with solidus temperatures of approximately 1530 K (for the Fe52.5Mo23.5Cr18.7C5.3 alloy) and 1525 K (for the Fe55.5Mo11.8Cr28.2C4.5 alloy) were revealed. The linear thermal expansion coefficients for the χ Fe,Cr,Mo,C, η Fe,Cr,Mo,C, and αFe,Cr,Mo,C phases of different composition observed for different temperature ranges were determined.
引用
收藏
页码:613 / 624
页数:11
相关论文
共 50 条
  • [1] High-Temperature Phases in the Fe-Mo-Cr-C System
    Velikanova, T. A.
    Zaslavskii, A. M.
    Kindrachuk, M. V.
    POWDER METALLURGY AND METAL CERAMICS, 2023, 61 (9-10) : 613 - 624
  • [2] Formation of active phases of Fe/C, Cr/C and Fe-Cr/C catalysts in oxidative dehydrogenation of ethane
    Mishanin, Igor I.
    V. Bogdan, Tatiana
    V. Smirnov, Aleksey
    Chernavskii, Petr A.
    Kuznetsova, Natalia N.
    Bogdan, Viktor I.
    MENDELEEV COMMUNICATIONS, 2023, 33 (03) : 422 - 424
  • [3] High-temperature gas corrosion of austenitic Cr – Ni steel containing Mo and Ti
    D. S. Stavrev
    Ts. D. Dikova
    I. P. Ivanov
    Metal Science and Heat Treatment, 2012, 53 : 508 - 511
  • [4] Study on High-Temperature Interaction Mechanism of Nd-Fe-As System
    Fu, Chenghui
    Huang, Run
    Xie, Wenhao
    Luo, Jinxiao
    Li, Yulian
    Zhang, Jinzhu
    MATERIALS, 2019, 12 (19)
  • [5] High-Temperature Oxidation Behavior and Mechanism of a New Type of Wrought Ni–Fe–Cr–Al Superalloy up to 1300°C
    Jinfeng Huang
    Hongsheng Fang
    Xiaorong Fu
    Fuxiang Huang
    Hong Wan
    Qianfa Zhang
    Shiping Deng
    Jishseng Zu
    Oxidation of Metals, 2000, 53 : 273 - 287
  • [6] Effect of Si on High-Temperature Corrosion Resistance of Ni-Cr-Mo Alloy Cladding Layer
    Chen Shanshan
    Liu Zongde
    Pan Chaoyang
    Cheng Kehan
    Shen Yue
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (07) : 2343 - 2352
  • [7] High-Temperature Oxidation Behavior of Fe-10Cr Steel under Different Atmospheres
    Cheng, Lei
    Sun, Bin
    Du, Chongyang
    Gao, Wei
    Cao, Guangming
    MATERIALS, 2021, 14 (13)
  • [8] First-principles study of phase stability and temperature-dependent mechanical properties of (Cr, M)23C6 (M = Fe, Mo) phases
    Gong, Xiaoguo
    Cui, Can
    Yu, Qiang
    Wang, Wei
    Xu, Wei-Wei
    Chen, Lijie
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 824
  • [9] High-Temperature Oxidation and Wear Behavior of (Fe,Cr)Al Intermetallic Compound and (Fe,Cr)Al-Al2O3 Nanocomposites
    Sourani, F.
    Enayati, M. H.
    Taghipour, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (05) : 3654 - 3669
  • [10] Precipitation and phase transformation behavior during high-temperature aging of a cobalt modified Fe-24Cr-(22-x)Ni-7Mo-xCo superaustenitic stainless steel
    Liao, Luhai
    Li, Jingyuan
    Zhao, Zhengxiang
    Xu, Fanghong
    Zhang, Wei
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (07) : 4771 - 4788