High-Temperature Oxidation of FeCr(Ni) Alloys: The Behaviour After Breakaway

被引:0
作者
T. Jonsson
H. Larsson
S. Karlsson
H. Hooshyar
M. Sattari
J. Liske
J.-E. Svensson
L.-G. Johansson
机构
[1] Chalmers University of Technology,Environmental Inorganic Chemistry, Department of Chemistry and Chemical Engineering
[2] Thermo-Calc Software,undefined
来源
Oxidation of Metals | 2017年 / 87卷
关键词
High-temperature oxidation; Breakaway corrosion; Stainless steel; Internal oxidation;
D O I
暂无
中图分类号
学科分类号
摘要
The oxidation of an austenitic FeCr(Ni) steel at 600 °C in H2O + KCl + O2/H2 + H2O + Ar environments is studied up to 168 h. The oxidation behaviour after “breakaway” is investigated by microstructural investigations, and thermodynamic calculations (Thermo-Calc) on the FeCr(Ni)–O system are used to interpret the results. The characteristic “breakaway” scale morphology exhibits an outward-growing iron oxide and a bottom layer consisting of inward-growing spinel oxide and reaction zones containing Cr-rich oxide precipitates and Cr-depleted metal. The equilibrium calculations show that a miscibility gap appears in the FeCr spinel oxide below 665 °C influencing the microstructure of the inward-growing scale. Equilibrium calculations on the FeCrNi–O system show that Ni is not expected to enter the spinel oxide in low oxygen activity conditions, in accordance with observations.
引用
收藏
页码:333 / 341
页数:8
相关论文
共 29 条
[1]  
Pujilaksono B(2011)undefined Oxidation of Metals 75 183-207
[2]  
Hansson AN(2010)undefined Oxidation of Metals 73 289-309
[3]  
Essuman E(2007)undefined Scripta Materialia 57 845-848
[4]  
Young DJ(2011)undefined Corrosion Science 53 2131-2141
[5]  
Meier GH(2010)undefined Oxidation of Metals 74 319-340
[6]  
Andersson JO(2002)undefined Calphad 26 273-312
[7]  
Sundman B(1991)undefined Journal of Phase Equilibria 12 127-140
[8]  
Asteman H(2000)undefined Oxidation of Metals 54 11-26
[9]  
Pujilaksono B(2011)undefined Oxidation of Metals 75 183-207
[10]  
Othman NK(2009)undefined Corrosion Science 51 3039-3049