H2S Poisoning and Regeneration of a Nickel Spinellized Catalyst Prepared from Waste Metallurgical Residues, During Dry Autothermal Methane Reforming

被引:0
作者
Frank Blondel Dega
Nicolas Abatzoglou
机构
[1] Université de Sherbrooke,Department of Chemical Engineering and Biotechnological Engineering
来源
Catalysis Letters | 2019年 / 149卷
关键词
Spinel; Regeneration; Nickel; Calcination; Deactivation;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:1730 / 1742
页数:12
相关论文
共 116 条
[1]  
Bychkov VY(2011)Carbonization of nickel catalysts and its effect on methane dry reforming Appl Catal A Gen 453 71-79
[2]  
Tyulenin YP(2016)H Can J Chem Eng 94 650-654
[3]  
Firsova AA(2010)S poisoning of NiAl Ind Eng Chem Res 49 10144-10148
[4]  
Shafranovsky EA(2019)O Renew Energy 138 1239-1249
[5]  
Gorenberg AY(2018)/Al Energy Convers Manage 171 133-155
[6]  
Korchak VN(2011)O Chin J Catal 32 273-279
[7]  
Blanchard J(2018)-YSZ catalyst during methane dry reforming Catal Sci Technol 8 1578-1588
[8]  
Achouri I(2014)Regeneration of sulfur deactivated Ni-based biomass syngas cleaning catalysts Energy Fuels 28 2104-2113
[9]  
Abatzoglou N(2018)Autothermal dry reforming of methane with a nickel spinellized catalyst prepared from a negative value metallurgical residue Catalysts 8 12-F213
[10]  
Li L(2013)A review of recent developments in hydrogen production via biogas dry reforming J Electrochem Soc 161 F208-280