Electrical and electrochemical characteristics of La0.6Sr0.4CoO3-δ cathode materials synthesized by a modified citrate-EDTA sol-gel method assisted with activated carbon for proton-conducting solid oxide fuel cell application

被引:0
作者
Abdullah Abdul Samat
Abdul Azim Jais
Mahendra Rao Somalu
Nafisah Osman
Andanastuti Muchtar
Kean Long Lim
机构
[1] Universiti Kebangsaan Malaysia,Fuel Cell Institute
[2] Universiti Teknologi MARA,Faculty of Applied Sciences
[3] Universiti Kebangsaan Malaysia,Centre for Materials Engineering and Smart Manufacturing (MERCU), Faculty of Engineering and Built Environment
来源
Journal of Sol-Gel Science and Technology | 2018年 / 86卷
关键词
Solid oxide fuel cell; LSC cathode; Activated carbon; Sol-gel; Electrical properties;
D O I
暂无
中图分类号
学科分类号
摘要
The electrical conductivity and electrochemical performance of a La0.6Sr0.4CoO3-δ (LSC) cathode produced by a modified citrate-EDTA sol-gel method assisted with activated carbon are characterized for a proton-conducting solid oxide fuel cell (H+ −SOFC) application at intermediate temperature. Thermogravimetric analysis revealed that the decomposition of the unrequired intermediate compounds in the precalcined powder was completed at 800 °C. A single LSC perovskite phase was formed at a calcination temperature of 900 °C, as confirmed by X-ray diffraction analysis. The particle size, crystallite size, and BET-specific surface area of the powder are 219–221 nm, 18 nm, and 9.87 m2 g−1, respectively. The high index value of the extent of agglomeration (5.53) showed that the powder was barely agglomerated. Bulk LSC sintered at 1200 °C for 2 h showed the highest direct-current electrical conductivity (σd.c) compared to that of bulk LSC sintered at 1000 °C and 1100 °C. The value of σd.c was affected by the density and porosity of the sintered samples. The area specific resistance (ASR) of screen-printed LSC working on a proton conductor of BaCe0.54Zr0.36Y0.1O2.95 (BCZY) decreased from 5.0 Ω cm2–0.06 Ω cm2 as the temperature increased from 500 °C to 800 °C with an activation energy of 1.079 eV. Overall, in this work, the LSC material produced with the aid of activated carbon meet the requirements for the application as a cathode in an intermediate temperature H+-SOFC.
引用
收藏
页码:617 / 630
页数:13
相关论文
共 216 条
[1]  
Garbayo I(2014)undefined J Power Sources 248 1042-1049
[2]  
Esposito V(2010)undefined J Power Sources 195 6709-6718
[3]  
Sanna S(2011)undefined J Power Sources 196 7263-7270
[4]  
Morata A(2012)undefined Electrochem Solid-State Lett 15 B54-B56
[5]  
Pla D(2012)undefined J Power Sources 209 172-179
[6]  
Fonseca L(2016)undefined J Sol-Gel Sci Technol 78 187-194
[7]  
Sabate N(2016)undefined J Sol-Gel Sci Technol 80 259-266
[8]  
Tarancon A(2010)undefined Int J Hydrog Energy 35 9411-9419
[9]  
Heel A(2016)undefined Malays J Anal Sci 20 1458-1466
[10]  
Holtappels P(2016)undefined Solid State Sci Technol 24 135-142