- [2] Mould filling of low-pressure expendable pattern casting process for magnesium alloys Huazhong Ligong Daxue Xuebao, 2006, 11 (19-21):
- [3] Expendable pattern casting of AZ91D magnesium alloy THERMEC'2003, PTS 1-5, 2003, 426-4 : 623 - 628
- [4] Mold-filling characteristics and solidification behavior of magnesium alloy in vacuum suction casting process Journal of Materials Science, 2009, 44 : 5644 - 5653
- [7] Effect of process parameters on density of magnesium alloy parts by low-pressure expendable pattern casting TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S358 - S362