Feasibility study on contact heating warm forming of 7075-T6 aluminum alloy

被引:3
作者
Sun, Lu [1 ,2 ]
Zhang, Zhiqiang [1 ,2 ]
Song, Zhenkun [1 ,2 ]
Ren, Mingwen [1 ,2 ]
Jia, Hongjie [1 ,2 ]
机构
[1] Jilin Univ, Key Lab Automobile Mat, Minist Educ, 5988 Renmin St, Changchun 130022, Peoples R China
[2] Jilin Univ, Sch Mat Sci & Engn, 5988 Renmin St, Changchun 130022, Peoples R China
关键词
7075 aluminum alloy; Contact heating warm forming; Microstructures; Mechanical properties; FORMABILITY; PRECIPITATION; SHEET; STRENGTH;
D O I
10.1007/s43452-023-00749-w
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
7075 aluminum alloy is becoming an ideal material for the manufacture of vehicle body parts due to the demands for energy-saving and lighter vehicles. To solve the problem that the strength of 7075-T6 aluminum alloy decreases due to over-aging after warm forming, contact heating warm forming (CHWF) technology was proposed in this work. Contact heating is a fast and efficient heating method that can make the blank reach the target temperature in a very short time. In this work, the effect of contact heating on the mechanical properties and microstructures of 7075-T6 aluminum alloy after warm forming and paint-baking (PB) was studied. It only took about 11.5 s to heat the 2 mm 7075 aluminum alloy sheet to 200 celcius by contact heating, and the strength and the hardness of the formed parts could reach 94% and 92.5% of T6 condition, respectively. In contrast, the heating furnace needed 690 s to heat the sheet to 200 & DEG;C, and the strength and the hardness of the formed parts were 87% and 85.4% of T6 condition, respectively. Due to the fast heating rate of contact heating (17.5 celcius/s), the atoms and vacancies in the matrix did not have time to undergo diffusion and aggregation, so that the precipitates could not coarsen obviously. As a result, most of the & eta;' precipitates in the T6 condition were retained. However, long-term heating in the furnace led to the transformation of & eta;' precipitates into coarse & eta; phase and the loss of strength and hardness.
引用
收藏
页数:8
相关论文
共 50 条
[31]   The effect of impulses on precipitation behavior in 7075-T6 aluminum alloy joint by impulse friction stir welding [J].
Keqi Wang ;
Anton Naumov ;
Marina Gushchina ;
Fedor Isupov ;
Ahmad Alali Alkhalaf ;
Oleg Panchenko .
The International Journal of Advanced Manufacturing Technology, 2023, 128 :373-389
[32]   Investigation of the friction and wear properties of nitrided 7075-T6 aluminum alloy under vacuum and ambient air [J].
Ghahramanzadeh Asl, Hojjat ;
Sert, Yasar ;
Bayrak, Ozgu ;
Kucukomeroglu, Tevfik .
PAMUKKALE UNIVERSITY JOURNAL OF ENGINEERING SCIENCES-PAMUKKALE UNIVERSITESI MUHENDISLIK BILIMLERI DERGISI, 2022, 28 (01) :63-71
[33]   Enhancement of the delamination resistance of adhesive film coated surface laser melted aluminum 7075-T6 alloy by aminophosphonic acid adsorption [J].
Vieth, P. ;
Garthe, M. -A. ;
Voswinkel, D. ;
Schaper, M. ;
Grundmeier, G. .
SURFACE & COATINGS TECHNOLOGY, 2022, 447
[34]   Role of Ultrasonic Shot Peening in Environmental Hydrogen Embrittlement Behavior of 7075-T6 Alloy [J].
Safyari, Mahdieh ;
Moshtaghi, Masoud .
HYDROGEN, 2021, 2 (03) :377-385
[35]   Effects of the local microstructures on the mechanical properties in FSWed joints of a 7075-T6 Al alloy [J].
Lee, WB ;
Lee, CY ;
Yeon, YM ;
Jung, SB .
ZEITSCHRIFT FUR METALLKUNDE, 2005, 96 (08) :940-947
[36]   Ultrasonic and Conventional Fatigue Endurance of Aeronautical Aluminum Alloy 7075-T6, with Artificial and Induced Pre-Corrosion [J].
Zuniga Tello, Ishvari F. ;
Milkovic, Marijana ;
Dominguez Almaraz, Gonzalo M. ;
Gubeljak, Nenad .
METALS, 2020, 10 (08) :1-17
[37]   Influence of reversible and non-reversible fatigue on the microstructure and mechanical property evolution of 7075-T6 aluminum alloy [J].
Indeck, Joseph ;
Demeneghi, Gabriel ;
Mayeur, Jason ;
Williams, Cyril ;
Hazeli, Kavan .
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 145
[38]   THE EFFECT OF ELECTROLYTE TEMPERATURE AND SEALING SOLUTION IN ANODIZING OPERATION ON HARDNESS AND WEAR BEHAVIOR OF 7075-T6 ALUMINUM ALLOY [J].
Niyazbakhsh, Saeed ;
Amini, Kamran ;
Gharavi, Farhad .
SURFACE REVIEW AND LETTERS, 2019, 26 (02)
[39]   The effects of friction stir welding on microstructure and formability of 7075-T6 sheet [J].
Mehri, Ali ;
Abdollah-zadeh, Amir ;
Entesari, Sina ;
Saeid, Tohid ;
Wang, Jing Tao .
RESULTS IN ENGINEERING, 2023, 18
[40]   Retrogression and reaging of 7075 T6 aluminum alloy [J].
Fleck, P ;
Calleros, D ;
Madsen, M ;
Trinh, T ;
Hoang, D ;
Foyos, J ;
Lee, EW ;
Es-Said, OS .
ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 2000, 331-3 :649-654