Characterization of degradation and iron deposits of the wood of Nanhai I shipwreck

被引:0
作者
Hongying Zhang
Dawa Shen
Zhiguo Zhang
Qinglin Ma
机构
[1] University of Science and Technology Beijing,Institute of Cultural Heritage and History of Science & Technology
[2] China Academy of Cultural Heritage,International Joint Research Laboratory of Environmental and Social Archaeology
[3] National Centre for Archaeology,undefined
[4] Shandong University,undefined
来源
Heritage Science | / 10卷
关键词
Nanhai I shipwreck; Marine archaeological wood; Waterlogged wood; Degradation; Iron deposits;
D O I
暂无
中图分类号
学科分类号
摘要
Nanhai I shipwreck was a large wooden merchant ship (22.15 m in length and 9.85 m in width) built in the Southern Song Dynasty (1127–1279 A.D.) of China, which was heavily loaded with a large number of porcelain and iron artifacts. In the South China Sea, it was found in 1987 and lifted as a whole in 2007. Its excavation provides a precious opportunity to reveal the preservation status of Nanhai I shipwreck. Iron compounds give rise to challenges in conservation procedures and the long-term stability of Nanhai I shipwreck. In this paper, the degradation of the wood and the iron deposits in the wood structure are investigated from the aspects of microscopic morphology, composition, and distribution to evaluate the preservation state of the waterlogged wood. Physical parameters, chemical composition, and the results of elemental analysis, and FTIR analysis suggest that the cellulose of wood is degraded, and the relative concentration of lignin increases. The ash content varies greatly among different samples, and the element of the highest content in ash is iron. The study on transverse and longitudinal sections from samples indicate that the deposits are unevenly concentrated in the cell lumen, middle lamella, rays, and pits of the cell wall. The cell lumen is filled with deposits in areas close to the surface of the samples. The XRD analysis demonstrates that the deposits in wood are mainly iron deposits, containing compounds pyrite (FeS2), siderite (FeCO3), iron oxyhydroxides (FeOOH), and magnetite (Fe3O4). The micro-X-ray Fluorescence mapping analysis suggests that the content of iron is relatively richer while containing less sulfur on the exterior of the sample. The presence of iron deposits accelerates wood degradation and increases the safety hazards of shipwrecks in the preservation process. We hope that our findings can make a modest contribution to iron removal from waterlogged archeological wood and shipwreck conservation.
引用
收藏
相关论文
共 131 条
[1]  
Sun J(2020)Archaeological summary of the Song Dynasty shipwreck Nanhai I in China Natl Mar Res 1 55-76
[2]  
Almkvist G(2011)Distribution of iron and sulfur and their speciation in relation to degradation processes in wood from the Swedish warship Vasa New J Chem 35 1491-1502
[3]  
Persson I(2003)Chemical characterisation of wood of Roman Ships brought to light in the recently discovered ancient Harbour of Pisa (Tuscany, Italy) Holzforschung 57 373-376
[4]  
Bettazzi F(1990)Conservation of waterlogged timbers from the Batavia 1629 Bull Aust Inst Marit Archaeol 14 1-8
[5]  
Giachi G(2019)Post-treatment study of Iron/Sulfur-containing compounds in the wreck of Lyon Saint-Georges 4 (Second Century ACE) Stud Conserv 65 28-36
[6]  
Staccioli G(2018)Study on wood preservation state of Chinese ancient shipwreck Huaguangjiao I J Cult Herit 32 53-59
[7]  
Chimichi S(2014)Analysis and research on the wood from the Ming Dynasty shipwreck, Nan'ao No.1, in Shantou city, Guangdong Sci Conserv Archaeol 26 30-38
[8]  
Macleod ID(2014)Research on the removal of the iron sulfides in the Qing Dynasty marine shipwreck, Ningbo Xiaobaijiao No. 1 Sci Conserv Archaeol. 62 57-63
[9]  
Rémazeilles C(2008)Polysaccharide degradation in waterlogged oak wood from the ancient warship Vasa Holzforschung 13 2521-2527
[10]  
Meunier L(2012)State of degradation in archeological oak from the 17th century Vasa ship: substantial strength loss correlates with reduction in (holo)cellulose molecular weight Biomacromol 58 297-307