Cavitation Erosion Behaviors of a Nickel-Free High-Nitrogen Stainless Steel

被引:0
|
作者
Yanxin Qiao
Zhaohui Tian
Xiang Cai
Jian Chen
Yuxin Wang
Qining Song
Huabing Li
机构
[1] Jiangsu University of Science and Technology,School of Materials Science and Engineering
[2] Suzhou Nuclear Research Institute,College of Mechanical and Electrical Engineering
[3] Hohai University,School of Metallurgy
[4] Northeastern University,undefined
来源
Tribology Letters | 2019年 / 67卷
关键词
High-nitrogen stainless steel; Cavitation erosion; Corrosion; Synergistic effect;
D O I
暂无
中图分类号
学科分类号
摘要
The cavitation erosion and corrosion characteristic of a nickel-free high-nitrogen stainless steel (HNSS) in distilled water and 0.5 mol/L HCl solution were investigated by conducting gravimetric and electrochemical measurements, including corrosion potential, polarization curves and electrochemical impedance spectroscopy, and the eroded/corroded surface was observed by scanning electron microscopy. The results revealed that the dominant contribution to cavitation erosion damage was the mechanical degradation process, even though the corrosion rate of HNSS was accelerated in 0.5 mol/L HCl solution. Corrosion and mechanical degradation worked synergistically and promoted crack initiation and propagation under cavitation erosion.
引用
收藏
相关论文
共 50 条
  • [42] High nitrogen nickel-free austenitic stainless steel: A promising coronary stent material
    Yang Ke
    Ren YiBin
    Wan Peng
    SCIENCE CHINA-TECHNOLOGICAL SCIENCES, 2012, 55 (02) : 329 - 340
  • [43] Preparation of high nitrogen and nickel-free austenitic stainless steel by powder injection molding
    Cui, Dawei
    Jiang, Junsheng
    Cao, Guangming
    Xiao, Enzhong
    Qu, Xuanhui
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2008, 15 (02): : 150 - 154
  • [44] High nitrogen nickel-free austenitic stainless steel: A promising coronary stent material
    Ke Yang
    YiBin Ren
    Peng Wan
    Science China Technological Sciences, 2012, 55 : 329 - 340
  • [45] Nanoindentation creep deformation behaviour of high nitrogen nickel-free austenitic stainless steel
    Zhang, Xiaoru
    Sun, Shicheng
    Sun, Guixun
    Han, Shuang
    Jiang, Zhonghao
    Lian, Jianshe
    MATERIALS SCIENCE AND TECHNOLOGY, 2019, 35 (13) : 1592 - 1599
  • [46] Kinetics of Cr2N Precipitation and Its Effect on Pitting Corrosion of Nickel-Free High-Nitrogen Austenitic Stainless Steel
    K. Krishna Kumar
    J. Anburaj
    R. Dhanasekar
    T. Satishkumar
    J. Abuthakir
    P. Manikandan
    R. Subramanian
    Journal of Materials Engineering and Performance, 2020, 29 : 6044 - 6052
  • [47] Discontinuous precipitation in a nickel-free high nitrogen austenitic stainless steel on solution nitriding
    Mohammadzadeh, Roghayeh
    Akbari, Alireza
    Grumsen, Flemming B.
    Somers, Marcel A. J.
    PHILOSOPHICAL MAGAZINE, 2017, 97 (30) : 2795 - 2814
  • [48] Kinetics of Cr2N Precipitation and Its Effect on Pitting Corrosion of Nickel-Free High-Nitrogen Austenitic Stainless Steel
    Krishna Kumar, K.
    Anburaj, J.
    Dhanasekar, R.
    Satishkumar, T.
    Abuthakir, J.
    Manikandan, P.
    Subramanian, R.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 6044 - 6052
  • [49] Physical simulation of the heat-affected zone in nickel-free high-nitrogen stainless steel weld at various peak temperatures and cooling rates
    Dhanasekar, R.
    Kumar, T. Satish
    Kumar, K. Krishna
    Jeyaprakash, N.
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [50] Cavitation erosion behavior of high-nitrogen austenitic stainless steel: Effect and design of grain-boundary characteristics
    Wang, Zhenhua
    Zhang, Bing
    MATERIALS & DESIGN, 2021, 201