Warm-temperature tensile ductility in Al-Mg alloys

被引:1
作者
Eric M. Taleff
Gregory A. Henshall
T. G. Nieh
Donald R. Lesuer
Jeffrey Wadsworth
机构
[1] University of Texas,the Department of Aerospace Engineering and Engineering Mechanics
[2] Hewlett-Packard Laboratories,Manufacturing and Materials Engineering Division
[3] the Lawrence Livermore National Laboratory,Science and Technology
[4] the Lawrence Livermore National Laboratory,undefined
[5] the Lawrence Livermore National Laboratory,undefined
来源
Metallurgical and Materials Transactions A | 1998年 / 29卷
关键词
Cavitation; Material Transaction; Tensile Ductility; Ternary Addition; Binary Material;
D O I
暂无
中图分类号
学科分类号
摘要
Several binary and ternary Al alloys containing from 2.8 to 5.5 wt pct Mg were tested in tension at elevated temperatures (200 °C to 500 °C) over a range of strain rates (10−4 to 2.0 s−1). Tensile ductilies of up to 325 pct were obtained in binary Al-Mg alloys with coarse grains deformed in the solute-drag creep regime. Under test conditions in which solute-drag creep controls deformation, Mg in concentrations from 2.8 to 5.5 wt pct neither affects tensile ductility nor influences strain-rate sensitivity or flow stress significantly. Strength is shown to increase with increasing Mg concentration, however, in the power-law-breakdown regime. The solute-drag creep process, which leads to superplastic-like elongations, is shown to have no observable grain-size dependence in a binary Al-Mg material. Ternary alloying additions of Mn and Zr are shown to decrease the strain-rate sensitivity during solute-drag creep, negatively influencing ductility. An important cause of reduced ductility in the ternary alloys during creep deformation is found to be a transition from necking-controlled failure in the binary alloys to cavitation-controlled failure in the ternary alloys investigated. An increase in ternary element concentration, which can increase the relative volume percentage of proeutectic products, increases cavitation.
引用
收藏
页码:1081 / 1091
页数:10
相关论文
共 86 条
[21]  
Horiuchi R.(1992)undefined Metall. Trans. A 23A 881-89
[22]  
Otsuka M.(1991)undefined Metall. Trans. A 22A 1037-47
[23]  
Linga Murty K.(1985)undefined Adv. Technol. Mater. Processes 30 994-1004
[24]  
Mohamed F.A.(1978)undefined Scripta Metall. 12 99-102
[25]  
Dorn J.E.(1979)undefined Metall. Trans. A 10A 41-46
[26]  
Orlová A.(1979)undefined Metall. Trans. A 10A 849-54
[27]  
Čadek J.(1991)undefined Mater. Sci. Eng. A132 97-105
[28]  
Oikawa H.(1969)undefined Met. Sci. J. 3 1-7
[29]  
Matsuno N.(1967)undefined Acta Metall. 15 351-55
[30]  
Karashima S.(1969)undefined Trans. Am. Soc. Met. 62 291-93