Effect of annealing on mechanical properties of silicon carbide sintered with aluminum nitride and scandium oxide

被引:0
作者
Shin-Il Ko
Sang-Jin Lee
Myong-Hoon Roh
Wonjoong Kim
Young-Wook Kim
机构
[1] Mokpo National University,Department of Advanced Materials Science and Engineering
[2] The University of Seoul,Department of Materials Science and Engineering
来源
Metals and Materials International | 2009年 / 15卷
关键词
ceramics; silicon carbide; microstructure; toughness; strength;
D O I
暂无
中图分类号
学科分类号
摘要
Beta-SiC powder samples containing 1 wt.% α-SiC as a seed and 10 vol.% AlN-Sc2O3 as a sintering additive were hot-pressed at 1900 °C for 1 h and subsequently annealed at 2000 °C for 1 h, 3 h and 6 h. When the annealing time was increased, the microstructure changed from equiaxed to elongated grains, which resulted in a self-reinforced microstructure consisting of elongated grains (hexagonal platelet grains in 3-dimensions). The development of a self-reinforced microstructure resulted in significant improvement in toughness. However, the improved toughness was offset by a reduction in strength. The typical fracture toughness and strength of the ceramics annealed for 6 h were 7.3 MPa·m1/2 and ∼500 MPa, respectively.
引用
收藏
页码:149 / 153
页数:4
相关论文
共 74 条
[1]  
Biswas K.(2004)undefined Mater. Sci. Eng. A. 374 56-undefined
[2]  
Rixecker G.(2007)undefined Acta mater. 55 727-undefined
[3]  
Aldinger F.(2007)undefined Met. Mater. Int. 13 197-undefined
[4]  
Kim Y.-W.(1999)undefined J. Mater. Sci. 34 1197-undefined
[5]  
Chun Y. S.(1998)undefined J. Am. Ceram. Soc. 81 3136-undefined
[6]  
Nishimura T.(1996)undefined J. Am. Ceram. Soc. 79 1611-undefined
[7]  
Mitomo M.(1997)undefined J. Am. Ceram. Soc. 80 99-undefined
[8]  
Lee Y. H.(2004)undefined Int. J. Ref. Mat. Hard Mater. 22 169-undefined
[9]  
Kim Y.-W.(2005)undefined J. Am. Ceram. Soc. 88 1115-undefined
[10]  
Chun Y. S.(2002)undefined J. Europ. Ceram. Soc. 22 1321-undefined