Dry Sliding Friction and Wear Properties of Ti–TiC Composite Foams Prepared by Spark Plasma Sintering and Dissolution Process

被引:0
作者
Fan Lv
Jie Zhang
Chunxin Pan
Nan Cao
Jian Cao
Jun Tian
Binna Song
机构
[1] Soochow University,
[2] School of Mechanical and Electrical Engineering,undefined
[3] Soochow University,undefined
[4] School of Iron and Steel,undefined
来源
Powder Metallurgy and Metal Ceramics | 2022年 / 61卷
关键词
Ti–TiC composite foams; spark plasma sintering and dissolution; friction; porosity;
D O I
暂无
中图分类号
学科分类号
摘要
Ti–TiC composite foams were prepared by combining different volume fractions of TiC (0, 5, 10, and 15 vol.%) with NaCl as a space holder (20, 40, and 60 vol.%) by using spark plasma sintering (SPS) and a dissolution process. The sintering properties (relative density, porosity and microhardness), pore structure, friction and wear properties of the prepared foams were systematically studied. The Ti–TiC composite foams sintered at 700°C had an average pore diameter of approximately 230 μm. The microhardness of the Ti–10 vol.% TiC was significantly higher than that of porous Ti, with values ranging between 360.72 and 490.12 HV0.2 recorded for the composite. The average coefficient of friction (COF) for the Ti–TiC composite foams was measured as 0.12–0.17 using a pin-on-disk tribometer. The lowest COF was obtained for a foam with a volume fraction of added NaCl (VNaCl) of 40%. The wear rate of the examined foams was inversely related to their porosity, and the addition of TiC particles significantly improved the wear resistance of the porous Ti. The foams with 10 vol.% TiC exhibited the highest wear resistance, with a COF of 0.1349 and a wear rate of 0.65 ⋅ 10–12 m3 · N–1 · m–1. The wear mechanism of the Ti–TiC composite foams was a combination of adhesive and abrasive wear.
引用
收藏
页码:316 / 327
页数:11
相关论文
共 39 条
  • [1] Jing-pu Z(2019)Effects of pore size and porosity of surface-modified porous titanium implants on bone tissue ingrowth Trans. Nonferr. Met. Soc. 29 2534-2545
  • [2] Liang-jian C(2021)Sintering properties of in situ Ti–TiB microlattices created by 3D extrusion printing of TiH J. Cent. South Univ. 28 1078-1088
  • [3] Dai-yuan C(2019) + TiB Int. J. Adv. Manufact. Technol. 102 1689-1701
  • [4] Chun-sheng C(2017) inks Leonardo Electr. J. Pract. Technol. 16 269-286
  • [5] Man-fei Y(2019)Titanium-based matrix composites reinforced with particulate, microstructure, and mechanical properties using spark plasma sintering technique: a review Trans. Nonferr. Met. Soc. China 29 1653-1664
  • [6] Bo Z(2010)Processing of pure titanium containing titanium-based reinforcing ceramics additives using spark plasma sintering Adv. Eng. Mater. 12 863-872
  • [7] Song B(2016)Wear modes in open porosity titanium matrix composites with TiC addition processed by spark plasma sintering Trans. Nonferr. Met. Soc. China 26 348-358
  • [8] Cao J(1953)Spark plasma sintering, microstructures, and mechanical properties of macroporous titanium foams J. Appl. Phys. 24 981-988
  • [9] Falodun OE(2011)Effects of reinforcement on wear resistance of aluminum matrix composites Wear 272 88-96
  • [10] Obadele BA(2017)Contact and rubbing of flat surfaces Adv. Powder Technol. 28 1564-1572