The influence on the structure of Fe2+ → Mg substitution was studied in synthetic single crystals belonging to the MgCr2O4–FeCr2O4 series produced by flux growth at 900–1200 °C in controlled atmosphere. Samples were analyzed by single-crystal X-ray diffraction, electron microprobe analyses, optical absorption-, infrared- and Mössbauer spectroscopy. The Mössbauer data show that iron occurs almost exclusively as IVFe2+. Only minor Fe3+ (<0.005 apfu) was observed in samples with very low total Fe. Optical absorption spectra show that chromium with few exceptions is present as a trivalent cation at the octahedral site. Additional absorption bands attributable to Cr2+ and Cr3+ at the tetrahedral site are evident in spectra of end-member magnesiochromite and solid-solution crystals with low ferrous contents. Structural parameters a0, u and T–O increase with chromite content, while the M–O bond distance remains nearly constant, with an average value equal to 1.995(1) Å corresponding to the Cr3+ octahedral bond distance. The ideal trend between cell parameter, T–O bond length and Fe2+ content (apfu) is described by the following linear relations: a0=8.3325(5) + 0.0443(8)Fe2+ (Å) and T–O=1.9645(6) + 0.033(1)Fe2+ (Å) Consequently, Fe2+ and Mg tetrahedral bond lengths are equal to 1.998(1) Å and 1.965(1) Å, respectively.
引用
收藏
页码:633 / 642
页数:9
相关论文
共 50 条
  • [21] Raman study of MgCr2O4–Fe2+Cr2O4 and MgCr2O4–MgFe23+O4 synthetic series: the effects of Fe2+ and Fe3+ on Raman shifts
    Davide Lenaz
    Vanni Lughi
    Physics and Chemistry of Minerals, 2013, 40 : 491 - 498
  • [22] MgCr2O4 and MgCr2O4/Ag nanostructures: Facile size-controlled synthesis and their photocatalytic performance for destruction of organic contaminants
    Abbasi, Ali
    Sajadi, Seyed Milad Safar
    Amiri, Omid
    Hamadanian, Masood
    Moayedi, Hossein
    Salavati-Niasari, Masoud
    Beigi, Mandi Mohammad
    COMPOSITES PART B-ENGINEERING, 2019, 175
  • [23] INFLUENCE OF OXYGEN ACTIVITY ON SINTERING OF MGCR2O4
    ANDERSON, HU
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1974, 57 (01) : 34 - 37
  • [24] Why ion irradiation does not lead to the same structural changes in normal spinels ZnAl2O4, MgAl2O4 and MgCr2O4?
    Baldinozzi, G.
    Simeone, D.
    Gosset, D.
    Surble, S.
    Mazerolles, L.
    Thome, L.
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2008, 266 (12-13): : 2848 - 2853
  • [25] The reaction MgCr2O4 + SiO2 = Cr2O3 + MgSiO3 and the free energy of formation of magnesiochromite (MgCr2O4)
    Stephan Klemme
    Hugh S. C. O'Neill
    Contributions to Mineralogy and Petrology, 1997, 130 : 59 - 65
  • [26] SERIES MGCR2O4-MGFE2O4
    ALLEN, WC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1968, 51 (09) : 485 - &
  • [27] INFLUENCE OF OXYGEN ACTIVITY ON SINTERING OF MGCR2O4
    STEIN, JH
    ANDERSON, HU
    AMERICAN CERAMIC SOCIETY BULLETIN, 1972, 51 (09): : 722 - &
  • [28] KINETICS OF FORMATION OF MGCR2O4 IN THE SOLID-STATE AND ITS CHARACTERIZATION
    SHARMA, IB
    BATRA, S
    JOURNAL OF THE INDIAN CHEMICAL SOCIETY, 1988, 65 (04) : 243 - 244
  • [29] Synthesis and characterisation of MgCr2O4 spinel precursor
    Adhikari, UB
    Saha, MB
    Parya, TK
    JOURNAL OF THE INDIAN CHEMICAL SOCIETY, 2005, 82 (11) : 994 - 999
  • [30] Emergence of Highly Degenerate Excited States in the Frustrated Magnet MgCr2O4
    Tomiyasu, K.
    Yokobori, T.
    Kousaka, Y.
    Bewley, R. I.
    Guidi, T.
    Watanabe, T.
    Akimitsu, J.
    Yamada, K.
    PHYSICAL REVIEW LETTERS, 2013, 110 (07)