Abrasion of Al2O3–SiC–(Al, Si) composites made by melt oxidation

被引:0
作者
R. Arvind Singh
V. Jayaram
S. K. Biswas
机构
[1] Indian Institute of Science,Department of Mechanical Engineering
[2] Indian Institute of Science,Department of Metallurgy
来源
Journal of Materials Research | 1999年 / 14卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
We report here the remarkable abrasion wear resistance (normal pressure: 2.92 to 5.42 MPa; sliding speed: 0.25 to 3 m/s) of a soft (relative to other structural ceramics) melt-oxidized ceramic matrix composite Al2O3 –SiC–(Al, Si). In spite of being half as hard and more porous than zirconia toughened alumina (ZTA), a common cutting tool material, this composite fabricated at 1100 °C shows wear resistance comparable to that of ZTA at sliding speeds more than 2 m/s. The ability of this composite to generate a metal-rich tribofilm when rubbed and its high thermal shock resistance are factors which may be responsible for this unique performance.
引用
收藏
页码:64 / 67
页数:3
相关论文
共 33 条
[1]  
Newkirk MS(1986)undefined J. Mater. Res 1 81-1891
[2]  
Urquhart AW(1993)undefined J. Am. Ceram. Soc 76 1777-772
[3]  
Zwicker HR(1994)undefined Acta Metall. Mater 42 649-224
[4]  
Breval E(1996)undefined J. Am. Ceram. Soc 79 1881-128
[5]  
Manor E(1996)undefined J. Am. Ceram. Soc 79 770-89
[6]  
Ni H(1997)undefined J. Am. Ceram. Soc 80 219-3604
[7]  
Levi CG(1991)undefined Ceram. Eng. Sci. Proc 12 2203-undefined
[8]  
Mehrabian R(1996)undefined J. Am. Ceram. Soc 79 121-undefined
[9]  
Dhandapani SP(1994)undefined Wear 171 77-undefined
[10]  
Jayaram V(1990)undefined J. Mater. Sci 25 3592-undefined