Microstructure features of failure and mechanical properties of ultra-fine grained Ti-6AL-4V ELI alloy at 300-77 K

被引:6
作者
Tabachnikova E.D. [1 ]
Bengus V.Z. [1 ]
Podolskiy A.V. [1 ]
Smirnov S.N. [1 ]
Csach K. [2 ]
Miskuf J. [2 ]
Saitova L.R. [3 ]
Semenova I.P. [3 ]
Valiev R.Z. [3 ]
机构
[1] B. Verkin Institute for Low Temperature Physics and Engineering, Kharkov 61103, 47, Lenin Ave.
[2] Institute of Experimental Physics, Slovak Academy of Sciences, 043 53 Kosice
[3] Institute of Physics of Advanced Materials, USATU, Ufa 450000, 12, K. Marx Str.
关键词
ECAP; Failure regularities; Tensile testing; Ti-6Al-4V ELI alloy; Ultra dispersed structures;
D O I
10.1007/s10999-007-9036-0
中图分类号
学科分类号
摘要
Experimental investigation of mechanical characteristics and failure regularities of the ultra-fine grained Ti-6Al-4V ELI alloy, produced by equal channel angular pressing (ECAP), have been carried out under the uniaxial tension at 300 and 77 K. These characteristics have been compared for the different structural states of the Ti-6Al-4V ELI alloy, distinguished by the average grain size and by the morphology of α and β phases. It has been established that the combination of the heat treatment, ECAP, and the extrusion of the Ti-6Al-4V ELI alloy leads to a considerable increase of the alloy's strength in comparison with the initial state (54% at 300 K and 78% at 77 K) with preserving the reasonable values of the ductility (3-4% elongation to the neck beginning and 5-10% to the failure). For all investigated structural states of the Ti-6Al-4V ELI alloy only ductile failure was observed at 300 and 77 K. The fracture surface consists of regions failed under normal and shear stresses. In shear failure regions of fracture surface only elongated dimples were present. © 2007 Springer Science+Business Media B.V.
引用
收藏
页码:189 / 195
页数:6
相关论文
共 8 条
[1]  
Kim S.M., Kim J., Ko Y.G., Lee C.S., Shin D.H., Microstructure Development and segment formation during ECA pressing of Ti-6Al-4V alloy, Scripta Mater., 50, pp. 927-930, (2004)
[2]  
Liao S., Duffy J., Adiabatic shear bands in a Ti-6Al-4V titanium alloy, J. Mech. Phys. Solids., 46, pp. 2201-2231, (1998)
[3]  
Margolin H., Mahajan Y., Void formation, void growth and tensile fracture in Ti-6Al-4V, Metall. Trans. A, 9, pp. 781-791, (1978)
[4]  
Semenova I.P., Saitova L.R., Raab G.I., Valiev R.Z., Effect of severe plastic deformation on mechanical properties and structure of Ti alloys, Proceedings of the 8th ESAFORM Conference on Material Forming, 2, pp. 661-664, (2005)
[5]  
Semenova I.P., Saitova L.R., Raab G.I., Korshunov A.I., Zhu Y.T., Lowe T.C., Valiev R.Z., Microstructural features and mechanical properties of the Ti-6Al-4V ELI alloy processed by severe plastic deformation, Proceedings of the International Conference "nanomaterials by Severe Plastic Deformation", pp. 757-762, (2005)
[6]  
Stolyarov V.V., Zhu Y.T., Alexandrov I.V., Lowe T.C., Valiev R.Z., Refinement and properties of pure Ti processed by warm ECAP and cold rolling, Mater. Sci. Eng., 343, pp. 43-50, (2003)
[7]  
Tabachnikova E., Bengus V., Natsik V., Csach K., Miskuf J., Stolyarov V., Valiev R., Yntian Zhu T., Varyukhin V., Deformation and failure of Ti-6Al-4V nanostructured alloy at 300-4.2 K, Nanostructured Materials by High-Pressure Severe Plastic Deformation, pp. 259-263, (2006)
[8]  
Weiss I., Semiatin S.L., Thermomechanical processing of alpha titanium alloys-an overview, Mater. Sci. Eng., 263, pp. 243-256, (1999)