Vacancy cluster in ZnO films grown by pulsed laser deposition

被引:0
作者
Zilan Wang
Caiqin Luo
W. Anwand
A. Wagner
M. Butterling
M. Azizar Rahman
Matthew R. Phillips
Cuong Ton-That
M. Younas
Shichen Su
Francis Chi-Chung Ling
机构
[1] The University of Hong Kong,Department of Physics
[2] Institute of Radiation Physics,School of Mathematical and Physical Sciences
[3] Helmholtz-Zentrum Dresden-Rossendorf,PGG
[4] University of Technology Sydney,Institute of Optoelectronic Material and Technology
[5] Physics Division,undefined
[6] PINSTECH,undefined
[7] South China Normal University,undefined
来源
Scientific Reports | / 9卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Undoped and Ga-doped ZnO films were grown on c-sapphire using pulsed laser deposition (PLD) at the substrate temperature of 600 °C. Positron annihilation spectroscopy study (PAS) shows that the dominant VZn-related defect in the as-grown undoped ZnO grown with relative low oxygen pressure P(O2) is a vacancy cluster (most likely a VZn-nVO complex with n = 2, 3) rather than the isolated VZn which has a lower formation energy. Annealing these samples at 900 °C induces out-diffusion of Zn from the ZnO film into the sapphire creating the VZn at the film/sapphire interface, which favors the formation of vacancy cluster containing relatively more VZn. Increasing the P(O2) during growth also lead to the formation of the vacancy cluster with relatively more VZn. For Ga-doped ZnO films, the oxygen pressure during growth has significant influence on the electron concentration and the microstructure of the VZn-related defect. Green luminescence (GL) and yellow luminescence (YL) were identified in the cathodoluminescence study (CL) study, and both emission bands were quenched after hydrogen plasma treatment. The origin of the GL is discussed.
引用
收藏
相关论文
共 79 条
  • [1] Özgür Ü(2005)A comprehensive review of ZnO materials and devices J. Appl. Phys. 98 11-630
  • [2] McCluskey MD(2009)Defects in ZnO J. Appl. Phys. 106 10-1983
  • [3] Jokela S(2004)P‐type doping and devices based on ZnO Phys. Stat. Sol. (b) 241 624-22
  • [4] Look DC(2012)p-Type conductivity in n-doped ZnO: the role of the N Phys. Rev. Lett. 108 215501-224
  • [5] Claflin B(2013)– V Appl. Phys. Lett. 102 152114-101
  • [6] Liu L(2003) complex Phys. Rev. Lett. 91 205502-undefined
  • [7] Reynolds J(2011)Shallow acceptor complexes in p-type ZnO Phys. Rev. B 84 115202-undefined
  • [8] Tuomisto F(2004)Evidence of the Zn vacancy acting as the dominant acceptor in n-type ZnO Phys. Rev. Lett. 92 155504-undefined
  • [9] Ranki V(2018)Self-compensation in semiconductors: The Zn vacancy in Ga-doped ZnO J. Appl. Phys. 123 161525-undefined
  • [10] Saarinen K(2009)Doping by large-size-mismatched impurities: the microscopic origin of arsenic-or antimony-doped p-type zinc oxide Phys. Rev. B 80 035331-undefined