The influence of aging on the fracture load of milled monolithic crowns

被引:0
作者
Ceyda Güleç
Işıl Sarıkaya
机构
[1] Tokat Gaziosmanpasa University,Department of Prosthodontics, Faculty of Dentistry
来源
BMC Oral Health | / 22卷
关键词
CAD/CAM; Chewing simulator; Aging; Fracture load; Monolithic crowns;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
相关论文
共 146 条
[1]  
Sjogren G(2000)Cytotoxicity of dental alloys, metals, and ceramics assessed by millipore filter, agar overlay, and MTT tests J Prosthet Dent 84 229-236
[2]  
Sletten G(2007)Achieving natural-looking morphology and surface textures in anterior ceramic fixed rehabilitations Int J Periodontics Restorative Dent 7 117-125
[3]  
Dahl JE(2015)Fracture strength of aged monolithic and bilayer zirconia-based crowns Biomed Res Int. 1 1-7
[4]  
Gallucci GO(2014)Influence of veneer and cyclic loading on failure behavior of lithium disilicate glass-ceramic molar crowns Dent Mater 30 164-171
[5]  
Guex P(2016)Fracture-resistant monolithic dental crowns Dent Mater 32 442-449
[6]  
Vinci D(2015)Mechanical properties of resin-ceramic CAD/CAM restorative materials J Prosthet Dent 114 587-593
[7]  
Belser UC(1995)Relative flexural strength of six new ceramic materials Int J Prosthodont 8 239-246
[8]  
Lameira DP(2013)Chair-side generated posterior lithium disilicate crowns after 4 years Clin Oral Investig 17 1765-1772
[9]  
Zhao K(2016)Polymer infiltrated ceramic network structures for resistance to fatigue fracture and wear Dent Mater 32 1352-1361
[10]  
Wei Y-R(2016)Fatigue resistance of CAD/CAM resin composite molar crowns Dent Mater 32 499-509