Semiconducting ceramics produced using nanocrystalline barium titanate powder

被引:0
作者
V. N. Shut
S. V. Kostomarov
机构
[1] Belarussian Academy of Sciences,Institute of Technical Acoustics
来源
Inorganic Materials | 2009年 / 45卷
关键词
Barium Titanate; Firing Temperature; Resistance Ratio; Electric Strength; Barium Titanate;
D O I
暂无
中图分类号
学科分类号
摘要
Positive temperature coefficient of resistance ceramics of composition (Ba0.89Ca0.08Pb0.03)TiO3 + Y2O3 + MnO + SiO2 have been produced using barium titanate powder with an average crystallite size of 125 nm prepared by calcining barium titanyl oxalate at 900°C. The effect of firing temperature on their microstructure and electrical properties has been studied. The results demonstrate that the ceramics possess semiconducting properties starting at a firing temperature of 1205–1215°C. The room-temperature resistivity of the ceramics has a minimum at tfiring ≈ 1245–1250°C. The samples sintered at 1250–1260°C have the largest positive temperature coefficient of resistance. The highest electric strength (360 V/mm at ρ25°C = 290 Ω cm) is offered by the thermistor materials sintered at 1260°C, which is 60–70°C below the firing temperature of analogous ceramics produced by solid-state reaction.
引用
收藏
页码:1417 / 1422
页数:5
相关论文
共 50 条