Correction to: High-Temperature Hydrogen Attack on 2.25Cr–1Mo Steel: The Roles of Residual Carbon, Initial Microstructure and Carbide Stability

被引:0
作者
M. A. M. Alshahrani
S. W. Ooi
M. Hörnqvist Colliander
G. M. A. M. El-Fallah
H. K. D. H. Bhadeshia
机构
[1] University of Cambridge,Materials Science and Metallurgy
[2] Saudi Aramco Research and Development Centre,Department of Physics
[3] Chalmers University of Technology,School of Engineering
[4] University of Leicester,School of Engineering and Materials Science
[5] Queen Mary University of London,undefined
来源
Metallurgical and Materials Transactions A | 2023年 / 54卷