Burial-induced deterioration in leather: a FTIR-ATR, DSC, TG/DTG, MHT and SEM study

被引:0
作者
Gabriela Vyskočilová
Cristina Carşote
Richard Ševčík
Elena Badea
机构
[1] Masaryk University,Department of Chemistry, Faculty of Science
[2] National Museum of Romanian History,Department of Chemistry, Faculty of Sciences
[3] Advanced Research for Cultural Heritage Group (ARCH Lab),undefined
[4] National Research & Development Institute for Textile and Leather,undefined
[5] ICPI Division,undefined
[6] University of Craiova,undefined
来源
Heritage Science | / 10卷
关键词
Vegetable tanned leather; Soil burial; Deterioration; FTIR-ATR; DSC; TG/DTG; SEM; MHT;
D O I
暂无
中图分类号
学科分类号
摘要
In this study we used an analytical approach based on complementary techniques that targets all structural levels of collagen in leather to investigate how vegetable-tanned leather deteriorates during soil burial tests. For the first time, a group of deterioration markers specific to molecular, fibrillar and fibrous structure of collagen in leather was associated with the deterioration of buried leather. The application of the second order derivative of FTIR-ATR spectra analysis allowed us to detect loosening of collagen–tannin matrix, de-tanning and gelatin formation based on the behaviour of collagen and tannin spectral components (intensity variation and shifts). Collagen denaturation observed by DSC analysis and its thermo-oxidative behaviour measured by TG/DTG analysis, as well as the altered morphology of collagen (namely melt-like fibres and distorted fibrillar ultrastructure) imaged by SEM confirmed the FTIR-ATR analyis results. These analytical outcomes enabled us to understand the effect of leather hardening/cementing through soil mineral penetration into its fibrous structure and thus correctly interprete the higher-than-expected shrinkage temperatures and intervals determinatd by MHT method. Thus, MHT method proved to be suitable for a quick evaluation method that can direcly support the first conservation decision after excavation. The combination of FTIR-ATR, DSC, TG/DTG and SEM can be particularly useful to provide insights on the deterioration mechanism of archaeological leather and support best decision on its long-term preservation.
引用
收藏
相关论文
共 186 条
  • [1] Rich A(1961)The molecular structure of collagen J Mol Biol 3 483-506
  • [2] Crick FHC(2009)Collagen structure and stability Annu Rev Biochem 78 929-958
  • [3] Shoulders MD(2006)Microfibrillar structure of type I collagen in situ Proc Natl Acad Sci USA 103 9001-9005
  • [4] Raines RT(2005)Prediction of collagen stability from amino acid sequence J Biol Chem 280 19343-19349
  • [5] Orgel JPRO(2006)Nature designs tough collagen: explaining the nanostructure of collagen fibrils Proc Natl Acad Sci USA 103 12285-12290
  • [6] Irving TC(1997)Modern tanning chemistry Chem Soc Rev 26 111-126
  • [7] Wess TJ(2016)Investigations towards the binding mechanisms of vegetable tanning agents to collagen Res J Phytochem 10 58-66
  • [8] Persikov AV(2008)Link-lock: an explanation of the chemical stabilisation of collagen J Soc Leather Technol Chem 92 1-7
  • [9] Ramshaw JA(2010)Microstructural, chemical and isotopic evidence for the origin of late neolithic leather recovered from an ice field in the Swiss Alps J Archaeol Sci 37 1851-1865
  • [10] Brodsky B(2019)Identifying archaeological leather—discussing the potential of grain pattern analysis and zooarchaeology by mass spectrometry (ZooMS) through a case study involving medieval shoe parts from Denmark J Cult Herit 39 21-31