Solvent-Free Manufacturing of Electrodes for Lithium-ion Batteries

被引:0
作者
Brandon Ludwig
Zhangfeng Zheng
Wan Shou
Yan Wang
Heng Pan
机构
[1] Missouri University of Science and Technology,Department of Mechanical and Aerospace Engineering
[2] Rolla,Department of Mechanical Engineering
[3] MO-65409,undefined
[4] US,undefined
[5] Worcester Polytechnic Institute,undefined
来源
Scientific Reports | / 6卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Lithium ion battery electrodes were manufactured using a new, completely dry powder painting process. The solvents used for conventional slurry-cast electrodes have been completely removed. Thermal activation time has been greatly reduced due to the time and resource demanding solvent evaporation process needed with slurry-cast electrode manufacturing being replaced by a hot rolling process. It has been found that thermal activation time to induce mechanical bonding of the thermoplastic polymer to the remaining active electrode particles is only a few seconds. Removing the solvent and drying process allows large-scale Li-ion battery production to be more economically viable in markets such as automotive energy storage systems. By understanding the surface energies of various powders which govern the powder mixing and binder distribution, bonding tests of the dry-deposited particles onto the current collector show that the bonding strength is greater than slurry-cast electrodes, 148.8 kPa as compared to 84.3 kPa. Electrochemical tests show that the new electrodes outperform conventional slurry processed electrodes, which is due to different binder distribution.
引用
收藏
相关论文
共 73 条
  • [1] Liu D(2014)An effective mixing for lithium ion battery slurries Adv. Chem. Eng. Sci. 4 515-528
  • [2] Ruffo R(2008)Electrochemical behavior of LiCoO Electrochem. Commun. 11 247-249
  • [3] Wessells C(2010) as aqueous lithium-ion battery electrodes J. Power Sources 195 6049-6054
  • [4] Huggins RA(2011)Effect of slurry preparation process on electrochemical performances of LiCoO J. Power Sources 196 9682-9688
  • [5] Cui Y(2014) composite electrode J. Appl. Electrochem. 44 209-214
  • [6] Lee G-W(2014)On the impact of the slurry mixing procedure in the electrochemical performance of composite electrodes for Li-ion batteries: A case study for mesocarbon microbeads (MCMB) graphite and Co J. Power Sources 256 28-31
  • [7] Ryu J-H(2008)O J. Electrochem. Soc. 155 A887-A892
  • [8] Han W(2010)A different method for producing a flexible LiMn Sci. Proc. Riga Tech. Univ. Ser. 1. 21 67-71
  • [9] Ahn KH(2014)O Ind. Eng. Chem. Res. 53 9094-9100
  • [10] Oh SM(2007)/MWCNT J. Power Sources 163 1047-1052