共 190 条
[1]
Jiang L(2007)Comparison of polylactide/nano-sized calcium carbonate and polylactide/montmorillonite composites: reinforcing effects and toughening mechanisms Polymer 48 7632-7644
[2]
Zhang JW(2019)Evaluation of commercially available polylactic acid (PLA) filaments for 3D printing applications J Therm Anal Calorim 137 555-562
[3]
Wolcott MP(2020)Influence of the combination of nucleating agent and plasticizer on the non-isothermal crystallization kinetics and activation energies of poly(lactic acid) J Therm Anal Calorim 139 1069-1090
[4]
Matos BDM(2007)Plastic deformation of amorphous poly(L/DL-lactide): structure evolution and physical properties Biomacromol 8 1836-1843
[5]
Rocha V(2011)Research progress in toughening modification of poly(lactic acid) J Polym Sci Pol Phys 49 1051-1083
[6]
Silva EJD(1987)Stereocomplex formation between enantiomeric poly(lactides) Macromolecules 20 904-906
[7]
Moro FH(1999)Stereocomplex formation between enantiomeric poly(lactic acid)s. XI. Mechanical properties and morphology of solution-cast films Polymer 40 6699-6708
[8]
Bottene AC(2020)Solid and microcellular polylactide nucleated with PLA stereocomplex and cellulose nanocrystals J Therm Anal Calorim 45 189-197
[9]
Ribeiro CA(2012)Temperature-variable FTIR and solid-state 13C NMR investigations on crystalline structure and molecular dynamics of polymorphic poly(L-lactide) and poly(L-lactide)/poly(D-lactide) stereocomplex Macromolecules 116 9983-9991
[10]
Dias DDS(2012)Investigation of poly(lactide) stereocomplexes: 3-armed poly(L-lactide) blended with linear and 3-armed enantiomers J Phys Chem B 210 993-1002