Hydration of alkali-activated ground granulated blast furnace slag

被引:1
作者
S. Song
D. Sohn
H. M. Jennings
T. O. Mason
机构
[1] Northwestern University,Department of Materials Science
[2] Northwestern University,Department of Materials Science and Engineering and Civil Engineering
来源
Journal of Materials Science | 2000年 / 35卷
关键词
Polymer; Microstructure; Aqueous Solution; Furnace; Hydration;
D O I
暂无
中图分类号
学科分类号
摘要
The hydration of ground granulated blast furnace slag (GGBFS) at 25 °C in controlled pH environments was investigated during 28 days of hydration. GGBFS was activated by NaOH, and it was found that the rate of reaction depends on the pH of the starting solution. The main product was identified as C-S-H, and, in the pastes with high pH, hydrotalcite was observed at later stages of hydration. The pH of the mixing solution should be higher than pH 11.5 to effectively activate the hydration of GGBFS. As deduced from very low electrical conductivity measurements, GGBFS pastes had very tortuous and disconnected pores. The effect of the pH of the aqueous solution on the composition, microstructure and properties of alkali-activated GGBFS pastes are also discussed.
引用
收藏
页码:249 / 257
页数:8
相关论文
共 80 条
[1]  
Uchigawa H.(1986)undefined Proceedings of the 8th International Congress on the Chemistry of Cement, Rio de Janeiro 3 249-556
[2]  
Hakkinen T.(1993)undefined Cem. Concr. Res. 23 407-V168
[3]  
Hakkinen T.(1993)undefined Cem. Concr. Res. 23 518-468
[4]  
Regourd M.(1983)undefined Cem. Concr. Res. 13 549-undefined
[5]  
Thomassin J. H.(1994)undefined Advanced. Cem. Bas. Mat. 1 178-undefined
[6]  
Ballif P.(1994)undefined Cem. Concr. Res. 24 1033-undefined
[7]  
Touray J. C.(1993)undefined Cem. Concr. Res. 23 1253-undefined
[8]  
Qing-hua C.(1992)undefined Cem. Concr. Res. 22 1216-undefined
[9]  
Sarkar S. L.(1995)undefined Cem. Concr. Res. 25 561-undefined
[10]  
Wang S. D.(1992)undefined J. Mater. Sci. 27 6204-undefined