Higher energy and safer sodium ion batteries via an electrochemically made disordered Na3V2(PO4)2F3 material

被引:0
作者
Guochun Yan
Sathiya Mariyappan
Gwenaelle Rousse
Quentin Jacquet
Michael Deschamps
Renald David
Boris Mirvaux
John William Freeland
Jean-Marie Tarascon
机构
[1] Collège de France,Chimie du Solide
[2] Réseau sur le Stockage Electrochimique de l’Energie (RS2E),Energie, UMR 8260
[3] Sorbonne Université - 4 Place Jussieu,CNRS, CEMHTI UPR3079
[4] Univ. Orléans,LRCS
[5] Université de Picardie Jules Verne,Advanced Photon Source
[6] Argonne National Laboratory,School of Metallurgy and Environment
[7] Central South University,undefined
来源
Nature Communications | / 10卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The growing need to store an increasing amount of renewable energy in a sustainable way has rekindled interest for sodium-ion battery technology, owing to the natural abundance of sodium. Presently, sodium-ion batteries based on Na3V2(PO4)2F3/C are the subject of intense research focused on improving the energy density by harnessing the third sodium, which has so far been reported to be electrochemically inaccessible. Here, we are able to trigger the activity of the third sodium electrochemically via the formation of a disordered NaxV2(PO4)2F3 phase of tetragonal symmetry (I4/mmm space group). This phase can reversibly uptake 3 sodium ions per formula unit over the 1 to 4.8 V voltage range, with the last one being re-inserted at 1.6 V vs Na+/Na0. We track the sodium-driven structural/charge compensation mechanism associated to the new phase and find that it remains disordered on cycling while its average vanadium oxidation state varies from 3 to 4.5. Full sodium-ion cells based on this phase as positive electrode and carbon as negative electrode show a 10–20% increase in the overall energy density.
引用
收藏
相关论文
共 56 条
  • [1] Dunn B(2011)Electrical energy storage for the grid: a battery of choices Science 334 928-935
  • [2] Kamath H(2011)Electrochemical energy storage for green grid Chem. Rev. 111 3577-3613
  • [3] Tarascon JM(2015)Towards greener and more sustainable batteries for electrical energy storage Nat. Chem. 7 19-29
  • [4] Yang ZG(2017)Sustainability and in situ monitoring in battery development Nat. Mater. 16 45-56
  • [5] Larcher D(2015)Review—practical issues and future perspective for Na-ion batteries J. Electrochem. Soc. 162 A2538-A2550
  • [6] Tarascon JM(2013)Room-temperature stationary sodium-ion batteries for large-scale electric energy storage Energy Environ. Sci. 6 2338-2360
  • [7] Grey C(2014)Research development on sodium-ion batteries Chem. Rev. 114 11636-11682
  • [8] Tarascon J(2013)Towards high energy density sodium ion batteries through electrolyte optimization Energy Environ. Sci. 6 2361-2369
  • [9] Kubota K(2016)Optimization of Na-ion battery systems based on polyanionic or layered positive electrodes and carbon anodes J. Electrochem. Soc. 163 A867-A874
  • [10] Komaba S(2013)A new high-energy cathode for a Na-ion battery with ultrahigh stability J. Am. Chem. Soc. 135 13870-13878