Effect of Growth Temperature on Morphological, Structural, and Optical Properties of ZnO Nanorods Using Modified Chemical Bath Deposition Method

被引:0
|
作者
Ahmed Fattah Abdulrahman
Sabah Mohammed Ahmed
Samir Mustafa Hamad
Azeez Abdullah Barzinjy
机构
[1] University of Zakho,Department of Physics, Faculty of Science
[2] University of Duhok,Department of Physics, College of Science
[3] Soran University,Scientific Research Centre
[4] Salahaddin University-Erbil,Department of Physics, College of Education
[5] Tishk International University,Physics Education Department, Faculty of Education
来源
Journal of Electronic Materials | 2021年 / 50卷
关键词
ZnO nanorods; growth temperature; modified CBD; optical properties; seed layer;
D O I
暂无
中图分类号
学科分类号
摘要
Zinc oxide (ZnO) nanorods (NRs) have been investigated as a function of different growth temperature using modified chemical bath deposition (M-CBD) method. In this study, air bubbles were utilized inside the growth solution as an original modified process. The synthesis of ZnO NRs was carried out through two steps. The first step was deposition of the ZnO seed layer on the glass substrate, while the second step was growing the ZnO NRs on the seeded substrate. The impacts of the growth temperature on the morphology and crystal structure of the ZnO samples were investigated using field emission scanning electron microscopy and x-ray diffraction. UV–Vis spectroscopy was also utilized to characterize the optical properties of the ZnO NRs. The results showed that the growth of the ZnO samples is a NRs-like shape. The ZnO samples possess the hexagonal wurtzite structure with high crystal quality, and no other phases from the impurity were observed. Additionally,the ZnO NRs were found to be well oriented along te (002) planes with diameters ranging from 71 nm to 328 nm and length from 294 nm to 2475 nm, while the aspect ratio was up to 25 with different growth temperatures. However, the UV–Vis spectrum showed that the optical transmittance of the ZnO NRs dropped from ~ 66% to ~ 3.3%, and the absorption band edge had been shifted to a lower-energy region as the growth temperature increased from 65°C to 95°C. This is possibly due to the scattering increase and absorption light from voids, grain size, and thickness of the ZnO NRs. Therefore, it has been demonstrated that the ZnO NRs grown by the M-CBD method at a growth temperature of 95°C gives the most favorable result, since the NRs possess the optimum, homogenous, and uniform distribution with a higher aspect ratio, crystal quality, crystal size, and band gap energy.
引用
收藏
页码:1482 / 1495
页数:13
相关论文
共 50 条
  • [41] Vertically aligned ZnO nanorods synthesized using chemical bath deposition method on seed-layer ZnO/polyethylene naphthalate (PEN) substrates
    Shabannia, R.
    Abu-Hassan, H.
    MATERIALS LETTERS, 2013, 90 : 156 - 158
  • [42] Synthesis of ZnO nanorods via chemical bath deposition method: The effects of physicochemical factors
    Poornajar, Mahshid
    Marashi, Pirooz
    Fatmehsari, Davoud Haghshenas
    Esfahani, Mohammadreza Kolandouz
    CERAMICS INTERNATIONAL, 2016, 42 (01) : 173 - 184
  • [43] NOVEL PROCESS USING OXYGEN AND AIR BUBBLING IN CHEMICAL BATH DEPOSITION METHOD FOR VERTICALLY WELL ALIGNED ARRAYS OF ZnO NANORODS
    Abdulrahman, A. F.
    Ahmed, S. M.
    Ahmed, N. M.
    Almessiere, M. A.
    DIGEST JOURNAL OF NANOMATERIALS AND BIOSTRUCTURES, 2016, 11 (04) : 1073 - 1082
  • [44] Effect of substrate temperature on the structural properties of ZnO nanorods
    Karakose, Ercan
    Colak, Hakan
    ENERGY, 2017, 141 : 50 - 55
  • [45] Effect of annealing on structural and optical properties of indium sulfide thin layers produced by chemical bath deposition method
    Mehdi Nasiri Sarvi
    Parisa Esmaili
    Somayeh Asgary
    Indian Journal of Physics, 2020, 94 : 1545 - 1552
  • [46] Effect of annealing on structural and optical properties of indium sulfide thin layers produced by chemical bath deposition method
    Nasiri Sarvi, Mehdi
    Esmaili, Parisa
    Asgary, Somayeh
    INDIAN JOURNAL OF PHYSICS, 2020, 94 (10) : 1545 - 1552
  • [47] Structural, morphological, optical, and photoluminescence properties of nanocrystalline PbS thin films grown by chemical bath deposition
    Rajathi, S.
    Kirubavathi, K.
    Selvaraju, K.
    ARABIAN JOURNAL OF CHEMISTRY, 2017, 10 (08) : 1167 - 1174
  • [48] Optical properties of ZnO nanorods realised by aqueous chemical growth
    Bekeny, C.
    Voss, T.
    Gutowski, J.
    Postels, B.
    Kreye, M.
    Waag, A.
    SUPERLATTICES AND MICROSTRUCTURES, 2007, 42 (1-6) : 398 - 402
  • [49] The Effect of Deposition Temperature on the Growth of ZnO Nanorods on Porous Silicon using Sol-gel Immersion Method
    Amizam, S.
    Mamat, M. H.
    Khusaimi, Z.
    Rafaie, H. A.
    Sahdan, M. Z.
    Abdullah, S.
    Rusop, M.
    NANOSCIENCE AND NANOTECHNOLOGY, 2009, 1136 : 676 - +
  • [50] Low temperature hydrothermal growth and optical properties of ZnO nanorods
    Yang, J. H.
    Zheng, J. H.
    Zhai, H. J.
    Yang, L. L.
    CRYSTAL RESEARCH AND TECHNOLOGY, 2009, 44 (01) : 87 - 91