Resistance of Austenitic Nitrogen Cr – Ni – Mn Steels to Microbiological Corrosion

被引:0
|
作者
L. M. Kaputkina
I. V. Smarygina
I. A. Borzenkov
A. L. Tarasov
A. G. Svyazhin
V. E. Kindop
机构
[1] NITU “MISiS,Federal Research Center “Biotechnologies” of the Russian Academy of Sciences
[2] ”,undefined
[3] S. N. Vinogradsky Institute of Microbiology,undefined
来源
关键词
chromium-nickel-manganese nitrogen steels; microbiological corrosion; bioactive environment; sulfate-reducing bacteria;
D O I
暂无
中图分类号
学科分类号
摘要
The resistance of high-strength corrosion-resistant nitrogen Cr – Ni – Mn steels to microbiological corrosion is investigated. It is shown that lowering of the nickel content and elevation of the content of manganese lowers the corrosion strength of the steels in a synthesized solution of sulfate-reducing bacteria, whereas the additions of copper and nitrogen raise this strength. Surface defects and roughness intensify localization of the corrosion damage and accelerate the corrosion process in the steels.
引用
收藏
页码:115 / 120
页数:5
相关论文
共 50 条
  • [1] Resistance of Austenitic Nitrogen Cr - Ni - Mn Steels to Microbiological Corrosion
    Kaputkina, L. M.
    Smarygina, I. V.
    Borzenkov, I. A.
    Tarasov, A. L.
    Svyazhin, A. G.
    Kindop, V. E.
    METAL SCIENCE AND HEAT TREATMENT, 2018, 60 (1-2) : 115 - 120
  • [2] Effect of N, Mo, and Si on Local Corrosion Resistance of Unstabilized Cr–Ni and Cr–Mn–Ni Austenitic Steels
    L. A. Pisarevskii
    G. A. Filippov
    A. A. Lipatov
    Metallurgist, 2016, 60 : 822 - 831
  • [3] Cr-Mn-Ni austenitic steels alloyed additionally with nitrogen
    OAO 'Zavod Dneprospetsstal'', Dnepropetrovsk, Ukraine
    Stal, 11 (78):
  • [4] Effect of N, Mo, and Si on Local Corrosion Resistance of Unstabilized Cr-Ni and Cr-Mn-Ni Austenitic Steels
    Pisarevskii, L. A.
    Filippov, G. A.
    Lipatov, A. A.
    METALLURGIST, 2016, 60 (7-8) : 822 - 831
  • [5] Corrosion cracking, structure and properties of hardened Cr-Mn austenitic steels with nitrogen
    Goykhenberg, Yu.N.
    Zhuravlev, L.G.
    Mirzayev, D.A.
    Zhuravleva, V.V.
    Silina, Ye.P.
    Vnukov, V.Yu.
    Physics of Metals and Metallography, 1988, 65 (06): : 83 - 89
  • [6] High-Temperature Strength of Austenitic Nitrogen Corrosion-Resistant Cr – Ni – Mn Steels with Copper Additive
    L. M. Kaputkina
    A. G. Svyazhin
    I. V. Smarygina
    V. E. Kindop
    Metal Science and Heat Treatment, 2018, 60 : 158 - 164
  • [7] High-Temperature Strength of Austenitic Nitrogen Corrosion-Resistant Cr - Ni - Mn Steels with Copper Additive
    Kaputkina, L. M.
    Svyazhin, A. G.
    Smarygina, I. V.
    Kindop, V. E.
    METAL SCIENCE AND HEAT TREATMENT, 2018, 60 (3-4) : 158 - 164
  • [8] Dynamic strain aging of austenitic high nitrogen Cr-Ni and Cr-Mn steels
    Ilola, R
    Kemppainen, M
    Hänninen, H
    HIGH NITROGEN STEELS '98, 1999, 318-3 : 407 - 412
  • [9] STUDY OF CORROSION CRACKING, STRUCTURE AND PROPERTIES OF STRENGTHENED CR-MN AUSTENITIC STEELS WITH NITROGEN
    GOYKHENBERG, YN
    ZHURAVLEV, LG
    MIRZAYEV, DA
    ZHURAVLEVA, VV
    SILINA, YP
    VNUKOV, VY
    FIZIKA METALLOV I METALLOVEDENIE, 1988, 65 (06): : 1131 - 1137
  • [10] Corrosion Properties of Austenitic Cr-Mn-Ni-N Steels with Various Manganese Concentrations
    Berezovskaya, V. V.
    Kostina, M. V.
    Blinov, E. V.
    Bannykh, I. O.
    Bobrova, V. E.
    Mel'nik, V. P.
    RUSSIAN METALLURGY, 2008, (01): : 29 - 33