Effect of Mg(OH)2 and sintering temperature on the hydration resistance of CaO aggregate by thermal decomposition

被引:0
作者
Tao Zhang
Yaowu Wei
Junfeng Chen
Nan Li
机构
[1] Wuhan University of Science and Technology,The State Key Laboratory of Refractories and Metallurgy
来源
Journal of the Australian Ceramic Society | 2020年 / 56卷
关键词
CaO aggregates; Density; Hydration resistance;
D O I
暂无
中图分类号
学科分类号
摘要
In spite of the advantages of CaO refractories, such as high refractoriness, potential to produce pure steel molten, and high alkaline corrosion resistance, their application has been limited due to its poor hydration resistance. Introducing additives to improve the hydration resistance of lime is a novel method. The influences of Mg(OH)2 and sintering temperatures on the sintering and hydration resistance of CaO aggregates that were produced by thermal decomposition were investigated in this paper. The purpose of this work was to produce high-purity CaO raw material with high density, low porosity, well grain growth, and good hydration resistance economically. The sintered samples were characterized by bulk density, apparent porosity, surface appearance, and microstructure. The results indicated that (1) Mg(OH)2 promoted the grain growth of CaO, reduced the apparent porosity, and improved the density of the specimens. The hydration resistance of the samples was increased. (2) Increasing the sintering temperature improved the hydration resistance of the specimens obviously in the experiment. (3) Grain size of CaO was more uniform with the increment of Mg(OH)2 content, and the density of the compacts was improved.
引用
收藏
页码:795 / 801
页数:6
相关论文
共 54 条
[1]  
Stendera JW(1956)Recent experience with dolomite in large steel ladles Iron and Steelmaker 13 3): 1-3):23
[2]  
Riedl JR(1985)Dolomite ladle refractories at inland steels no.1ElectricFurnace shop Iron and Steelmaker 12 44-45
[3]  
Tindyala MA(2004)The current status of tundish covering slags in a slab caster plant Metalurgija 43 59-62
[4]  
Brown Jesse J(2004)Relationship between clean steel and refractories Refractories 38 219-225
[5]  
Kijac J(2002)Refractories for clean steelmaking Am. Ceram. Soc. Bull. 81 32-35
[6]  
Kovac P(2003)Looking ahead—a new generation of high performance refractory ceramics Refractories 37 1-10
[7]  
Steranka E(1989)Preventives methods for hydration of calcia and dolomite clinker Taikabutsu 41 690-700
[8]  
Zhao-you C(2002)Carbonation of CaO clinkers and improvement of their hydration resistance Ceram Soc Japan 110 512-517
[9]  
Shou-xin T(2012)Effect of Fe J. Ceram. Process. Res. 13 646-650
[10]  
Wei YW(2016)O Ceram. Int. 42 12270-12275