- [1] Huang Q.-W.(2005)High-temperature strength and toughness behaviors for reaction-bonded SiC ceramics below 1400°C Mater. Lett 59 1732-1735
- [2] Zhu L.-H.(2019)Composite material for instrumental applications based on micro powder Al Int. J. Refract. Met. Hard Mater 82 336-339
- [3] Gevorkyan E.S.(2005)O Int. J. Appl. Ceram. Technol 1 56-67
- [4] Rucki M.(2021) with additives nano-powder SiC J. Instrum 16 P10015-78
- [5] Kagramanyan A.A.(2020)Biomorphic SiC: A new engineering ceramic material Materials 13 3768-33
- [6] Nerubatskiy V.P.(2021)Special features of manufacturing cutting inserts from nanocomposite material Al Nanomaterials 11 1351-144
- [7] Arellano-López A.R.(2017)O Adv. Mater. Sci. Eng 2017 2397238-117
- [8] Martínez-Fernández J.(2016)–SiC J. Mater. Sci. Chem. Eng 4 71-1583
- [9] González P.(2021)Effect of carbon addition and mixture method on the microstructure and mechanical properties of silicon carbide Materials 14 6503-62
- [10] Domínguez C.(2021)Behavior of silicon carbide materials under dry to hydrothermal conditions Materials 14 3432-46