摘要
Water degradation of glass waste forms has been studied extensively under a variety of conditions including of bulk glass immersed completely in static or dynamic water. In practice, the vitrified nuclear waste cracks as soon as poured into a container because of differences in thermal expansion coefficients. In addition, in repository the canisters may be only partially immersed in water. Later, water condenses on the surface of glass which corrodes releasing ions. In this work experiments have been performed to understand these effects on the degradation of International Simple Glass (ISG). Simulated cracks were found to develop pitting corrosion in the crack openings when tested by immersing ISG in water. Under load, these pits concentrated stress and grew as large planar cracks inside the glass. The condensation of water on glass surfaces leads to formation of pits and growth of calcium silicate crystals.
引用
收藏
页码:4215 / 4220
页数:5
相关论文
共 50 条
  • [21] Corrosion of the International Simple Glass under acidic to hyperalkaline conditions
    Backhouse, Daniel J.
    Fisher, Adam J.
    Neeway, James J.
    Corkhill, Claire L.
    Hyatt, Neil C.
    Hand, Russell J.
    NPJ MATERIALS DEGRADATION, 2018, 2 (01)
  • [22] Influence of young cement water on the corrosion of the International Simple Glass
    Colleen Mann
    Karine Ferrand
    Sanheng Liu
    Jeremy R. Eskelsen
    Eric Pierce
    Karel Lemmens
    Claire Corkhill
    npj Materials Degradation, 3
  • [23] Influence of young cement water on the corrosion of the International Simple Glass
    Mann, Colleen
    Ferrand, Karine
    Liu, Sanheng
    Eskelsen, Jeremy R.
    Pierce, Eric
    Lemmens, Karel
    Corkhill, Claire
    NPJ MATERIALS DEGRADATION, 2019, 3 (01)
  • [24] Application of GRAAL model to the resumption of International Simple Glass alteration
    Maxime Fournier
    Pierre Frugier
    Stéphane Gin
    npj Materials Degradation, 2
  • [25] OBSERVATION OF DUGDALE CRACKS IN GLASS FOILS - METHOD FOR STUDYING SURFACE PLASTICITY OF SODA-LIME GLASS
    SCHMIDT, V
    HOPFE, J
    JOURNAL OF MATERIALS SCIENCE, 1978, 13 (07) : 1599 - 1602
  • [26] SIMPLE APPROACH TO ESTIMATE SIZE OF SMALL SURFACE CRACKS WITH USE OF ACOUSTIC SURFACE-WAVES
    TITTMANN, BR
    COHENTENOUDJI, F
    DEBILLY, M
    JUNGMAN, A
    QUENTIN, G
    APPLIED PHYSICS LETTERS, 1978, 33 (01) : 6 - 8
  • [27] Effect of surface finish on strength degradation of glass ceramics
    Cao, YQ
    Zhang, GM
    ENGINEERING FAILURE ANALYSIS, 2000, 7 (01) : 11 - 26
  • [28] Degradation of the surface of a metasilicate glass due to atmosphere moisture
    Ziemath, EC
    QUIMICA NOVA, 1998, 21 (03): : 356 - 360
  • [29] SURFACE DEGRADATION OF E-GLASS AND S-GLASS IN PRESENCE OF WATER
    HSU, ACT
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1978, 176 (SEP): : 37 - 37
  • [30] Sub-surface cracks of borosilicate glass loaded by single grain of abrasive
    Dai, Zihua
    Zhu, Yongwei
    Ju, Zhilan
    Li, Jun
    Sun, Tao
    Zuo, Dunwen
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2014, 42 (09): : 1161 - 1166