Photocatalytic performance of PANI modified TiO2: Degradation of refractory organic matter

被引:0
|
作者
Ceyda S. Uyguner-Demirel
Nazli Turkten
Yunus Karatas
Miray Bekbolet
机构
[1] Bogazici University,Institute of Environmental Sciences
[2] Kirsehir Ahi Evran University,Department of Chemistry, Faculty of Arts and Sciences
来源
Environmental Science and Pollution Research | 2023年 / 30卷
关键词
Degradation kinetics; Photocatalysis; PANI-TiO; composite; Refractory organic matter;
D O I
暂无
中图分类号
学科分类号
摘要
Surface modification of TiO2 with polyaniline (PANI) conducting polymer has been used to achieve visible light photoresponse, thereby increasing solar photocatalytic activity. In this study, photocatalytic performances of PANI-TiO2 composites with different mole ratios were synthesized by the in situ chemical oxidation polymerization method and tested for the degradation of a model refractory organic matter (RfOM), namely humic acid in an aqueous medium under simulated solar irradiation in a comparative manner. Adsorptive interactions under dark conditions and interactions under irradiation were investigated as contributing factors to photocatalysis. Degradation of RfOM was monitored in terms of UV–vis parameters (Color436, UV365, UV280, and UV254) and fluorescence spectroscopic parameters as well as the mineralization extent by dissolved organic carbon contents. The presence of PANI exerted an enhancement in photocatalytic degradation efficiency compared to pristine TiO2. The synergistic effect was more pronounced in lower PANI ratios whereas higher PANI ratios reflected a retardation effect. Degradation kinetics were assessed by pseudo-first-order kinetic model. For all UV–vis parameters analyzed, highest and lowest rate constants (k) were attained in the presence of PT-14 (2.093 × 10−2 to 2.750 × 10−2 min−1) and PT-81 (5.47 × 10−3 to 8.52 × 10−3 min−1), respectively. Variations in selected absorbance quotients, i.e., A254/A436, A280/A436, and A253/A203, were distinctive and compared with respect to irradiation time and photocatalyst type. Upon use of PT-14, a steady decreasing profile with respect to irradiation time was attained for A253/A203 quotient as 0.76–0.61, followed by a rapid decrease to 0.19 in 120 min. The incorporation effect of PANI into TiO2 composite could be visualized in A280/A365 and A254/A365 quotients exhibiting an almost constant and parallel trend. As a general trend, decrease in the major fluorophoric intensity FIsyn,470 with photocatalysis was observed under extended irradiation conditions; however, an abrupt decline was remarkable in the presence of PT-14 and PT-18. Fluorescence intensity decrease correlated well with spectroscopic evaluation of rate constants. A thorough evaluation of spectroscopic parameters of UV–vis and fluorescence can provide significant information for practical applications in control of RfOM in water treatment.
引用
收藏
页码:85626 / 85638
页数:12
相关论文
共 50 条
  • [21] An insight into PANI-TiO2 photocatalysis of refractory organic matter through molecular size fractionation
    Uyguner-Demirel, Ceyda Senem
    Turkten, Nazli
    Bekbolet, Miray
    Environmental Science and Pollution Research, 2024, 31 (48) : 58335 - 58352
  • [22] CdS quantum dots confined in mesoporous TiO2 with exceptional photocatalytic performance for degradation of organic polutants
    Zhou, Panpan
    Xie, Yu
    Fang, Jing
    Ling, Yun
    Yu, Changling
    Liu, Xiaoming
    Dai, Yuhua
    Qin, Yuancheng
    Zhou, Dan
    CHEMOSPHERE, 2017, 178 : 1 - 10
  • [23] Plasma-Treated F modified TiO2 impact to enhance the photocatalytic performance of TiO2
    Yu, Bo
    Zhang, Lianhong
    Wu, Hongbo
    Wen, Jie
    Ali, Arshid Mahmood
    Zhang, Hui
    Zhang, Guoping
    Yu, Mingwei
    CHEMICAL PHYSICS LETTERS, 2022, 801
  • [24] Photocatalytic degradation of aqueous pollutants using silica-modified TiO2
    Vohra, MS
    Tanaka, K
    WATER RESEARCH, 2003, 37 (16) : 3992 - 3996
  • [25] Photocatalytic degradation of microcystin-LR by modified TiO2 photocatalysis: A review
    He, Xinghou
    Wang, Anzhi
    Wu, Pian
    Tang, Shibiao
    Zhang, Yong
    Li, Lei
    Ding, Ping
    SCIENCE OF THE TOTAL ENVIRONMENT, 2020, 743
  • [26] Surface-deposited nanofibrous TiO2 for photocatalytic degradation of organic pollutants
    Ruta Sidaraviciute
    Edvinas Krugly
    Lauryna Dabasinskaite
    Eugenijus Valatka
    Dainius Martuzevicius
    Journal of Sol-Gel Science and Technology, 2017, 84 : 306 - 315
  • [27] Photocatalytic degradation of nitrogen-containing organic compounds over TiO2
    Jing, Jieying
    Liu, Manhong
    Colvin, Vicki L.
    Li, Wenying
    Yu, William W.
    JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2011, 351 : 17 - 28
  • [28] Surface-deposited nanofibrous TiO2 for photocatalytic degradation of organic pollutants
    Sidaraviciute, Ruta
    Krugly, Edvinas
    Dabasinskaite, Lauryna
    Valatka, Eugenijus
    Martuzevicius, Dainius
    JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2017, 84 (02) : 306 - 315
  • [29] Photocatalytic Degradation of Methyl Orange with Commercial Organic Pigment Sensitized TiO2
    Shang, Xili
    Li, Bin
    Zhang, Tianyong
    Li, Changhai
    Wang, Xiao
    2013 INTERNATIONAL SYMPOSIUM ON ENVIRONMENTAL SCIENCE AND TECHNOLOGY (2013 ISEST), 2013, 18 : 478 - 485
  • [30] Selective photocatalytic degradation of organic pollutants by CuxS/ZnO/TiO2 heterostructures
    Isac, Luminita
    Andronic, Luminita
    Visa, Maria
    Enesca, Alexandru
    CERAMICS INTERNATIONAL, 2020, 46 (04) : 4265 - 4273