Water Vapor Effects on the CMAS Degradation of Thermal Barrier Coatings

被引:0
作者
B. S. Lutz
R. W. Jackson
N. M. Abdul-Jabbar
V. K. Tolpygo
C. G. Levi
机构
[1] University of California,Materials Department
[2] Santa Barbara,undefined
[3] Honeywell Aerospace,undefined
来源
Oxidation of Metals | 2017年 / 88卷
关键词
Thermal barrier coatings; CMAS; Thermally grown oxide; Spinel;
D O I
暂无
中图分类号
学科分类号
摘要
A new damage mechanism of CMAS degradation of TBCs involving delamination through the thermally grown oxide (TGO) has been observed on burner rig tests of EB-PVD thermal barrier coatings. This mechanism operates in the absence of CMAS melting and is mediated by hydroxylation and volatilization of the constituent CMAS hydroxides, followed by vapor transport to the vicinity of the TGO through the TBC porosity. Analyses reveal the formation of spinel (MgAl2O4) and anorthite (CaAl2Si2O8) at the TGO/TBC interface, with concomitant evolution of porosity at the spinel/alumina interface. Tests were conducted in a controlled atmosphere tube furnace to validate the hypothesis and assess the factors that affect the evolution of the deleterious oxides. The microstructure of the reaction products formed in the lab test is compared to that formed in the burner rig.
引用
收藏
页码:73 / 85
页数:12
相关论文
共 43 条
[1]  
Krämer S(2006)undefined Journal of the American Ceramic Society 89 3167-532
[2]  
Yang J(2012)undefined MRS Bulletin 37 932-undefined
[3]  
Levi CG(1996)undefined Surface and Coatings Technology 87 116-undefined
[4]  
Johnson CA(1992)undefined Geochimica et Cosmochimica Acta 56 511-undefined
[5]  
Levi CG(2013)undefined Annual Review of Materials Research 43 559-undefined
[6]  
Hutchinson JW(2009)undefined Calphad 33 295-undefined
[7]  
Vidal-Sétif MH(2003)undefined Zeitschrift fur Metallkunde 94 180-undefined
[8]  
Johnson CA(2013)undefined International Materials Reviews 58 63-undefined
[9]  
Borom MP(1998)undefined Earth and Planetary Science Letters 158 91-undefined
[10]  
Johnson CA(2014)undefined Acta Materialia 80 39-undefined