共 134 条
[1]
Ray RK(1994)Cold rolling and annealing textures in low carbon and extra low carbon steels Int. Metall. Rev. 39 129-undefined
[2]
Jonas JJ(1998)Physical parameters related to the developments of recrystallization textures in an ultra low carbon steel Acta Mater. 47 55-undefined
[3]
Hook RE(1997)Modeling of texture development during recrystallization of interstitial free steel Acta Mater. 45 2425-undefined
[4]
Samajdar I(2018)Effect of continuous annealing temperature on microstructure and properties of ferritic rolled interstitial-free steel Int. J. Miner. Metall. Mater. 25 536-undefined
[5]
Verlinden B(2008)Tensile behaviors of IF steel with different cold-rolling reductions Mater. Sci. Eng. A 496 383-undefined
[6]
Kestens L(2019)Comparison between the surface defects caused by Al Int. J. Miner. Metall. Mater. 26 178-undefined
[7]
Van Houtte P(2019)O Int. J. Miner. Metall. Mater. 26 440-undefined
[8]
Hayakawa Y(2017) and TiN inclusions in interstitial-free steel auto sheets Scripta Mater. 141 111-undefined
[9]
Szpunar JA(2016)Influence of metallurgical processing parameters on defects in cold-rolled steel sheet caused by inclusions Mater. Res. Lett. 4 145-undefined
[10]
Qiu CY(2007)Fabricating interstitial-free steel with simultaneous high strength and good ductility with homogeneous layer and lamella structure Mater. Sci. Eng. A 459 223-undefined