Effect of Slab Subsurface Microstructure Evolution on Transverse Cracking of Microalloyed Steel during Continuous Casting

被引:0
|
作者
Yun-feng Li
Guang-hua Wen
Ping Tang
Jian-quan Li
Cheng-li Xiang
机构
[1] Chongqing University,College of Materials Science and Engineering
[2] Pangang Group Panzhihua Steel and Vanagium Co.,undefined
[3] Ltd.,undefined
来源
Journal of Iron and Steel Research International | 2014年 / 21卷
关键词
continuous casting; microalloyed steel; surface transversal cracking; microstructure evolution; cooling pattern;
D O I
暂无
中图分类号
学科分类号
摘要
As to the continuous casting process of low carbon microalloyed steel, subsurface microstructure evolution plays an important role in the slab surface cracking. In order to study the effect of the slab subsurface microstructure evolution on the transverse cracking, three different secondary cooling patterns (i. e., mild cooling, strong cooling and controlled cooling) were performed in the corresponding slab curved continuous caster. Based on the metallographic results, three transformation regions were found to be formed with the evolution of microstructures at different depths in the slab subsurface. The three regions are strong cooling transformation (SCT) region, double phase transformation (DPT) region and mild cooling transformation (MCT) region, respectively. Meanwhile, it was also found that the crack index used for evaluating slab surface cracking susceptibility was decreased when the range of the DPT region was increased. This can be explained by the fact that the double phase transformation (austenite-ferrite-austenite) occurred resulting from thermal cycling in DPT region, which resulted in promoting the refinement of prior austenite grains and inhibiting the precipitation of film-like ferrite and chain-like precipitates. Under the controlled cooling pattern, the widely-distributed DPT region was formed in the range of 3.5 – 8.0 mm to the slab surface. And compared with other cooling patterns, the cracking susceptibility is lowest with a crack index of 0.4.
引用
收藏
页码:737 / 744
页数:7
相关论文
共 50 条
  • [31] Vanadium microalloyed steel for thin slab casting and direct rolling
    Li, Y
    Baker, TN
    MICROALLOYING FOR NEW STEEL PROCESSES AND APPLICATIONS, 2005, 500-501 : 237 - 243
  • [32] Vanadium Microalloyed Steel for Thin Slab Casting and Direct Rolling
    Li, Yu
    Milbourn, David
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 16 : 400 - 406
  • [33] Characteristic Parameters for Dendritic Microstructure of Solidification During Slab Continuous Casting
    Wei Guo
    Miao-yong Zhu
    Journal of Iron and Steel Research International, 2009, 16 : 17 - 21
  • [34] Characteristic Parameters for Dendritic Microstructure of Solidification During Slab Continuous Casting
    GUO Wei ZHU Miao-yong (School of Materials and Metallurgy
    Journal of Iron and Steel Research(International), 2009, 16 (01) : 17 - 21
  • [35] Evolution of substructure during continuous rolling of microalloyed steel strip
    Vodopivec, F
    Reskovic, S
    Mamuzic, I
    MATERIALS SCIENCE AND TECHNOLOGY, 1999, 15 (11) : 1293 - 1299
  • [36] The effect of coiling temperature on the microstructure and mechanical properties of a niobium-titanium microalloyed steel processed via thin slab casting
    Challa, V. S. A.
    Zhou, W. H.
    Misra, R. D. K.
    O'Malley, R.
    Jansto, S. G.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 595 : 143 - 153
  • [37] Characteristic Parameters for Dendritic Microstructure of Solidification During Slab Continuous Casting
    Guo Wei
    Zhu Miao-Yong
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 16 (01) : 17 - 21
  • [38] Research Mechanism of Formation on Transverse Corner Cracks in the Continuous Casting Slab of Peritectic Steel
    Zhou, Qinghai
    Yin, Yanbin
    Liu, Zhiming
    Zhang, Jiongming
    Zhang, Jiazheng
    STEEL RESEARCH INTERNATIONAL, 2022, 93 (11)
  • [39] Prevention of slab surface transverse cracking by microstructure control
    Kato, T
    Ito, Y
    Kawamoto, M
    Yamanaka, A
    Watanabe, T
    ISIJ INTERNATIONAL, 2003, 43 (11) : 1742 - 1750
  • [40] Research of 50Mn2V continuous casting slab transverse cracking during its retarded cooling process
    Wu, Maomeng
    Yu, Hao
    ENGINEERING FAILURE ANALYSIS, 2013, 30 : 61 - 73