Changes in microstructure and absorption-desorption pressures during hydrogen cycling in some intermetallic compounds

被引:0
|
作者
T. Yamamoto
M. Hirota
H. Inui
M. Yamaguchi
机构
[1] Kyoto University,Department of Materials Science and Engineering
来源
Metals and Materials | 2000年 / 6卷
关键词
LaNi; FeTi; hydrogen-storage alloy; dislocation; crack;
D O I
暂无
中图分类号
学科分类号
摘要
Changes in microstructure and their effects on hydrogen sorption properties have been investigated as a function of the number of hydrogen sorption cycles in LaNi5 and FeTi. For LaNi5, while the desorption pressure does not significandy depend on the number of cycles, the absorption pressure drastically decreases between the first and second cycles. In addition to severe cracking and pulverization, numerous edge dislocations with Burgers vectors of the l/3<1210>-type are introduced during the first absorption cycles. Both the introduction of numerous lattice defects and the formation of severe cracks seem to be completed during the first cycle, resulting in the reproducible P (pressure)-C (composition) characteristics for the subsequent cycles. In contrast, FeTi exhibits ever-changing P-C characteristics with cycle number. The introduction of dislocations with Burgers vectors of the <100>-type in the form of tangles and cracks occurs during each of absorption cycles with the extent to which this occurs being considerably smaller in each of absorption cycles of FeTi than in the first absorption cycle of LaNi5. The difference in material response to hydrogénation seems to be closely related to the difference in ductility of these two intermetallics.
引用
收藏
页码:609 / 615
页数:6
相关论文
共 50 条
  • [21] THE BEHAVIOR OF TI1.2CR1.9MN0.1 IN HYDROGEN ABSORPTION-DESORPTION CYCLING
    LUPU, D
    SARBU, R
    LUPU, R
    BIRIS, A
    CHIRIAC, G
    NEDA, A
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1988, 13 (04) : 239 - 242
  • [22] Local and crystal structure of Mg1.9Al0.1Ni hydrogen storage alloys during hydrogen absorption-desorption cycling
    Fan, Chao
    Ju, Xin
    Wan, Chubin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2010, 35 (15) : 8044 - 8048
  • [23] Structural change of NdNi3 during hydrogen absorption-desorption cycle
    Iwase, Kenji
    Mori, Kazuhiro
    Tashiro, Suguru
    Yokota, Hitoshi
    Suzuki, Tetsuya
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (06) : 3940 - 3945
  • [24] Hydrogen absorption and desorption properties of Hf-based intermetallic compounds
    Mukai, D
    Miyata, H
    Aoki, K
    JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 293 : 417 - 420
  • [25] CONTROL OF HYDROGEN ABSORPTION AND DESORPTION OF RARE-EARTH INTERMETALLIC COMPOUNDS
    GUALTIERI, DM
    NARASIMHAN, KSVL
    TAKESHITA, T
    JOURNAL OF APPLIED PHYSICS, 1976, 47 (08) : 3432 - 3435
  • [26] Microstructure of Hydrogenated Magnesium-Nickel Eutectic Alloy Based Composites and its Changes during Hydrogen Absorption/Desorption Cycling
    Fursikov, P. V.
    Fokin, V. N.
    Fokina, E. E.
    Arbuzov, A. A.
    Khodos, I. I.
    Lototskyy, M. V.
    Tarasov, B. P.
    HIGH ENERGY CHEMISTRY, 2023, 57 (SUPPL 2) : S310 - S315
  • [27] ABSORPTION-DESORPTION CHARACTERISTICS OF HYDROGEN FOR MMCO5
    KITADA, M
    JOURNAL OF MATERIALS SCIENCE, 1977, 12 (10) : 2134 - 2135
  • [28] CRITERIA FOR SUPERSATURATION DURING SIMULTANEOUS ABSORPTION-DESORPTION
    SHAH, YT
    JUVEKAR, VA
    SHARMA, MM
    CHEMICAL ENGINEERING SCIENCE, 1976, 31 (08) : 671 - 680
  • [29] Strain variation on the reaction tank of high hydrogen content during hydrogen absorption-desorption cycles
    Duan, Weiyuan
    Du, Junlin
    Wang, Zhenjie
    Niu, Yongqiang
    Huang, Tiesheng
    Li, Zhilin
    Pu, Chaohui
    Wu, Zhu
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (05) : 2347 - 2351
  • [30] Microstructure of Ti-V-Mn BCC alloys before and after hydrogen absorption-desorption
    Matsuda, Junko
    Nakamura, Yumiko
    Akiba, Etsuo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (11) : 4352 - 4356