Comparative Investigation and Characterization of the Scratch and Wear Resistance Behavior of TiN, CrN, AlTiN and AlCrN Cathodic Arc PVD Coatings

被引:1
作者
Akeem Yusuf Adesina
Zuhair M. Gasem
Abdul Samad Mohammed
机构
[1] King Fahd University of Petroleum and Minerals,Center of Research Excellence in Corrosion
[2] King Fahd University of Petroleum and Minerals,Mechanical Engineering Department
来源
Arabian Journal for Science and Engineering | 2019年 / 44卷
关键词
PVD coatings; Coefficient of friction; Scratch resistance; Wear; Tribology; Microindentation;
D O I
暂无
中图分类号
学科分类号
摘要
The scratch resistance and wear behavior at relatively high normal loads of binary (TiN, CrN) and ternary (Al0.50Ti0.50N, Al0.68Cr0.32N) coatings were comparatively investigated. Scratch test results showed that based on the adhesive strength the coatings can be ranked thus: CrN > TiN > Al0.68Cr0.32N > Al0.50Ti0.50N. The binary coatings were found to possess superior adhesion strength mainly exhibiting a tensile cracking failure mechanism. In contrast, the ternary coatings failed more severely by through-thickness cracking with spallation. The ternary coatings exhibited an average of 68, 67 and 55% improvement in the wear resistance at 15, 20 and 25 N normal loads, respectively, over the binary coatings. Abrasive and oxidation wear were the main wear mechanisms of the binary coatings. The formation of protective tribo-oxide layers is associated with the improved wear resistance behavior of the ternary coatings. High surface roughness due to large amount of surface defects coupled with low plastic deformation resistance and high Al content are reasons for low wear resistance of Al0.68Cr0.32N in comparison with Al0.50Ti0.50N coating.
引用
收藏
页码:10355 / 10371
页数:16
相关论文
共 165 条
[1]  
Mayrhofer PH(2006)Microstructural design of hard coatings Prog. Mater Sci. 51 1032-1114
[2]  
Mitterer C(2012)Hard nanocomposite coatings: thermal stability, oxidation resistance and toughness Surf. Coat. Technol. 207 50-65
[3]  
Hultman L(2014)Influence of Hf on the structure, thermal stability and oxidation resistance of Ti–Al–N coatings Thin Solid Films 565 25-31
[4]  
Clemens H(2014)Multilayer coatings based on CrN/Cr for molds of plastics Metall. Ital. 106 3-8
[5]  
Musil J(2014)The effect of increasing V content on the structure, mechanical properties and oxidation resistance of Ti–Si–V–N films deposited by DC reactive magnetron sputtering Appl. Surf. Sci. 289 114-123
[6]  
Xu YX(2014)Structure and property transitions of Al-based binary alloy coatings by magnetron sputtering Surf. Coat. Technol. 254 455-461
[7]  
Chen L(2017)Tribology of multilayer coatings for wear reduction: a review Friction 5 248-262
[8]  
Pei F(2014)Tribological properties of CrCN/CrN multilayer coatings Tribol. Int. 80 34-40
[9]  
Du Y(2014)Tribological behaviour at high temperature of hard CrAlN coatings doped with Y or Zr Thin Solid Films 550 413-420
[10]  
Liu Y(2010)Microstructure and mechanical properties of laser welded DP600 steel joints Mater. Sci. Eng., A 527 1215-1222