Microstructure evolution of carbidic austempered ductile iron at different austempering temperatures

被引:0
作者
Penghui Yang
Hanguang Fu
Rafik Absi
Rachid Bennacer
Moumen Darcherif
Shengqiang Ma
Jian Lin
Xingye Guo
机构
[1] Beijing University of Technology,Key Laboratory of Advanced Functional Materials, Ministry of Education, School of Materials Science and Engineering
[2] CY Cergy Paris University,Graduate School of Engineering
[3] ECAM-EPMI,School of Materials Science and Engineering
[4] Xi’an Jiaotong University,undefined
来源
Journal of Materials Science | 2021年 / 56卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
This work aims to elucidate the microstructure characteristics of each phase in carbidic austempered ductile iron and the nucleation and growth of acicular ferrite in an austempering temperature range of 250–450 °C. The research results showed that the carbides (Fe, Cr)3C obtained by the eutectic reaction had high indentation hardness and indentation modulus, and the interface between acicular ferrite and eutectic carbides belonged to incoherent boundary. Since the nucleation driving force of acicular ferrite increased with an increase in temperature difference (ΔT), the size of acicular ferrite gradually decreased with the decrease in isothermal temperature. When the austempering temperature was above 400 °C, acicular ferrite preferentially nucleated around the graphite nodules and inside grains. However, acicular ferrite preferentially nucleated around the graphite nodules and the eutectic carbides at temperature below 400 °C. Additionally, a fine twin structure had been found inside some acicular ferrite after austempering at a low temperature (250 °C).
引用
收藏
页码:4843 / 4857
页数:14
相关论文
共 137 条
  • [1] Laino S(2008)Development of wear resistant carbidic austempered ductile iron (CADI) Wear 265 1-7
  • [2] Sikora JA(2020)A REVIEW: phase transformation and wear mechanisms of single-step and dual-step austempered ductile irons J Mater Res Technol 9 1054-1069
  • [3] Dommarco RC(2011)Advances in the development of carbidic ADI Key Eng Mater 457 187-192
  • [4] Wang B(2010)Study of dry and minimum quantity lubrication drilling of novel austempered ductile iron (ADI) for automotive applications Wear 12 2412-2416
  • [5] Barber G(2014)Solid particle erosion behavior of carbidic austempered ductile iron modified by nanoscale ceria particles Mater Des 10 367-374
  • [6] Qiu F(2001)Development of austempered ductile cast iron (ADI) with simultaneous high yield strength and fracture toughness by a novel two-step austempering process Mater Sci Eng A 315 70-80
  • [7] Zou Q(2015)Effects of molybdenum on the wear resistance and corrosion resistance of carbidic austempered ductile iron Metallogr Microstruct Anal 4 298-304
  • [8] Yang H(2019)Effects of niobium alloying on microstructure, toughness and wear resistance of austempered ductile iron Mater Sci Eng A 760 186-194
  • [9] Laino S(2012)Influence of cooling rate on the microstructure and properties of a new wear resistant carbidic austempered ductile iron Mater Charact 72 53-58
  • [10] Sikora JA(2013)Modification of carbidic austempered ductile iron with nano ceria for improved mechanical properties and abrasive wear resistance Wear 301 116-121