Evaluation of the marginal adaptation and debonding strength of two types of CAD-CAM implant-supported cement-retained crowns

被引:0
作者
Nada Ahmed Ramzy
Amir Shoukry Azer
Mohamed Moataz Khamis
机构
[1] Alexandria University,Faculty of Dentistry
[2] Alexandria University,Department of Conservative Dentistry, Faculty of Dentistry
[3] Alexandria University,Department of Prosthodontics, Faculty of Dentistry
来源
BMC Oral Health | / 23卷
关键词
Abutment; Ceramics; Crown; Implant; Lithium disilicate; Polymers; Composite; Marginal fit; Adaptation; Margin; Debonding;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
相关论文
共 178 条
[1]  
Spitznagel FA(2018)CAD-CAM ceramic restorative materials for natural teeth J Dent Res. 97 1082-1091
[2]  
Boldt J(2017)Chair-side generated posterior monolithic lithium disilicate crowns: clinical survival after 6 years Clin Oral Investig. 21 2083-2089
[3]  
Gierthmuehlen PC(2015)Clinical evaluation of 121 lithium disilicate all-ceramic crowns up to 9 years Quintessence Int. 46 189-197
[4]  
Rauch A(2016)Influence of screw access channel on all ceramic cement-retained implant supported posterior crowns Int J of Science and Research. 5 2252-2258
[5]  
Reich S(2014)Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review J Prosthet Dent. 112 22-30
[6]  
Schierz O(2016)Ceramic-reinforced polymers: CAD/CAM hybrid restorative materials Curr Oral Health Rep. 3 198-202
[7]  
Toman M(2015)Mechanical properties of resin-ceramic CAD/CAM restorative materials J Prosthet Dent. 114 587-593
[8]  
Toksavul S(2020)Evaluation of the repair capacities and color stabilities of a resin nanoceramic and hybrid CAD/CAM blocks J Adv Prosthodont. 12 140-149
[9]  
Khalifa AE(2013)Mechanical properties of polymer-infiltrated-ceramic-network materials Dent Mater. 4 419-426
[10]  
Mostafa D(2015)Mechanical performance of implant-supported posterior crowns J Prosthet Dent. 114 59-66