Impact properties of carbon fibers-epoxy composite/aluminum laminates: effect of cryogenic and thermal aging

被引:0
作者
Mohammad Askari
Mehrdad Javadi
Reza Eslami-Farsani
Abdolreza Geranmayeh
机构
[1] South Tehran Branch,Department of Mechanical Engineering
[2] Islamic Azad University,Faculty of Materials Science and Engineering
[3] K.N. Toosi University of Technology,undefined
来源
Iranian Polymer Journal | 2023年 / 32卷
关键词
Thermal aging; Cryogenic aging; Environmental effect; Fiber/metal laminate; Impact strength;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:187 / 201
页数:14
相关论文
共 127 条
[1]  
Ebrahimnezhad-Khaljiri H(2017)Thermal and mechanical properties of hybrid carbon/oxidized polyacrylonitrile fibers-epoxy composites Polym Compos 38 1412-1417
[2]  
Eslami-Farsani R(2021)Mechanical properties of MWCNTs and graphene nanoparticles modified glass fibre-reinforced polymer nanocomposite Bull Mater Sci 44 194-214
[3]  
Turaka S(2020)Influence of seawater ageing on fracture of carbon fiber reinforced epoxy composites for ocean engineering Oceans 1 198-1969
[4]  
Reddy KVK(2018)Effect of nanoclay addition on the hygrothermal durability of glass/epoxy and fiber metal laminates Fibers Polym 19 1956-1554
[5]  
Sahu RK(2019)Effect of salt water conditioning on novel fiber metal laminates for marine applications Proc Inst Mech Eng Part L J Mater Des Appl 233 1542-195
[6]  
Katiyar JK(2020)Influence of flexible molecular structure on the cryogenic mechanical properties of epoxy matrix and carbon fiber/epoxy composite laminate Mater Des 195 188-194
[7]  
Le Guen-Geffroy A(2016)Hydrothermal aging of carbon reinforced epoxy laminates with nanofibrous mats as toughening interlayers Polym Degrad Stab 126 189-1431
[8]  
Davies P(2005)Ageing of a carbon epoxy composite for aeronautic applications Compos B 36 2006-171
[9]  
Le Gac PY(2021)Effect of thermal ageing on the mechanical strength of carbon fibre reinforced epoxy composites Polymers 13 2028-389
[10]  
Habert B(2020)Effect of exposure temperature on thecrashworthiness of carbon/epoxy compositerectangular tubes under quasi-static compression Polymers 12 1427-22