Influence of Gas Atmosphere Dew Point on the Selective Oxidation and the Reactive Wetting During Hot Dip Galvanizing of CMnSi TRIP Steel

被引:0
作者
Lawrence Cho
Seok Jae Lee
Myung Soo Kim
Young Ha Kim
Bruno C. De Cooman
机构
[1] Pohang University of Science and Technology,Materials Design Laboratory, Graduate Institute of Ferrous Technology
[2] POSCO Technical Research Laboratories,undefined
来源
Metallurgical and Materials Transactions A | 2013年 / 44卷
关键词
Internal Oxidation; Trip Steel; Intercritical Annealing; Reactive Wetting; Inhibition Layer;
D O I
暂无
中图分类号
学科分类号
摘要
The selective oxidation and reactive wetting of intercritically annealed Si-bearing CMnSi transformation-induced plasticity steels were investigated by high-resolution transmission electron microscopy. In a N2 + 10 pct H2 gas atmosphere with a dew point (DP) ranging from 213 K to 278 K (−60 °C to 5 °C), a continuous layer of selective oxides was formed on the surface. Annealing in a higher DP gas atmosphere resulted in a thinner layer of external oxidation and a greater depth of internal oxidation. The hot dipping was carried out in a Zn bath containing 0.22 mass pct Al, and the bath temperature was 733 K (460 °C). Coarse and discontinuous Fe2Al5−xZnx grains and Fe-Zn intermetallics (ζ and δ) were observed at the steel/coating interface after the hot dip galvanizing (HDG) of panels were annealed in a low DP atmosphere 213 K (−60 °C). The Fe-Zn intermetallics were formed both in areas where the Fe2Al5−xZnx inhibition layer had not been formed and on top of non-stoichiometric Fe-Al-Zn crystals. Poor wetting was observed on panels annealed in a low DP atmosphere because of the formation of thick film-type oxides on the surface. After annealing in higher DP gas atmospheres, i.e., 263 K and 278 K (−10 °C and 5 °C), a continuous and fine-grained Fe2Al5−xZnx layer was formed. No Fe-Zn intermetallics were formed. The small grain size of the inhibition layer was attributed to the nucleation of the Fe2Al5−xZnx grains on small ferrite sub-surface grains and the presence of granular surface oxides. A high DP atmosphere can therefore significantly contribute to the decrease of Zn-coating defects on CMnSi TRIP steels processed in HDG lines.
引用
收藏
页码:362 / 371
页数:9
相关论文
共 22 条
  • [21] Challenges in hot-dip galvanizing of high strength dual phase steel: Surface selective oxidation and mechanical property degradation
    Liu, Huachu
    Li, Fang
    Shi, Wen
    Swaminathan, Srinivasan
    He, Yanlin
    Rohwerder, Michael
    Li, Lin
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (16) : 3428 - 3436
  • [22] Selective Oxidation of a 0.1C-6Mn-2Si Third Generation Advanced High-Strength Steel During Dew-Point Controlled Annealing
    Pourmajidian, Maedeh
    McDermid, Joseph R.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (05): : 1795 - 1808