Effect of Flash Temperature on Tribological Properties of Bulk Metallic Glasses
被引:0
|
作者:
Jian Kong
论文数: 0引用数: 0
h-index: 0
机构:Nanjing University of Science and Technology,Department of Materials Science and Engineering
Jian Kong
Dangsheng Xiong
论文数: 0引用数: 0
h-index: 0
机构:Nanjing University of Science and Technology,Department of Materials Science and Engineering
Dangsheng Xiong
Jianliang Li
论文数: 0引用数: 0
h-index: 0
机构:Nanjing University of Science and Technology,Department of Materials Science and Engineering
Jianliang Li
Qunxing Yuan
论文数: 0引用数: 0
h-index: 0
机构:Nanjing University of Science and Technology,Department of Materials Science and Engineering
Qunxing Yuan
Rajnesh Tyagi
论文数: 0引用数: 0
h-index: 0
机构:Nanjing University of Science and Technology,Department of Materials Science and Engineering
Rajnesh Tyagi
机构:
[1] Nanjing University of Science and Technology,Department of Materials Science and Engineering
来源:
Tribology Letters
|
2009年
/
35卷
关键词:
Bulk metallic glass;
Friction and wear;
Flash temperature;
Nanocrystalline;
D O I:
暂无
中图分类号:
学科分类号:
摘要:
The tribological properties of Cu-based and Zr-based bulk metallic glasses (BMGs) sliding against Si3N4 under dry and water lubrication were studied on a pin-on-disc tribometer. The wear mechanisms of bulk metallic glasses were investigated based on the calculated flash temperature. The friction coefficients if fully amorphous alloy are about 0.7, while those of BMGs with nanocrytalline are a little higher. The wear rates of Cu-based BMG (V101) are about one order of magnitude lower than those of Zr-based BMG (Vit1) under dry friction, even two orders of magnitude lower under water lubrication. The wear resistance of bulk metallic glasses was influenced by the flash temperature. The calculated flash temperature (3,337 K) on the friction surface of Zr-based amorphous alloy exceeds its glass transition temperature, even its melting temperature. The high flash temperature leads to glass transition accompanied with viscous flow and material transfer, which is responsible for the poor wear resistance of Zr-based BMGs.