Effect of pediatric drugs on the color stability of dental restorative materials currently used in pediatric dentistry

被引:0
作者
Belen Şirinoğlu Çapan
Sinem Birant
机构
[1] Istanbul University-Cerrahpaşa,Faculty of Dentistry, Department of Paediatric Dentistry
来源
Journal of the Australian Ceramic Society | 2024年 / 60卷
关键词
Alkasite; Color stability; Glass ionomer cement; Pediatric drugs;
D O I
暂无
中图分类号
学科分类号
摘要
The purpose of this in vitro study was to assess the color stability of esthetic restorative materials after immersion in different pediatric drugs. Three different restorative materials namely composite resin, alkasite and high-viscosity glass ionomer cement(HVGIC) were used to prepare total 96 (32 from each) disc-shaped specimens(2mmx5mm). A spectrophotometer was used to record the color of each sample after sample preparation and 7 days following the staining technique. After 1-week period, ΔE ∗ values were calculated. The average color changes(ΔE) for all drugs/restorative materials ranged from 1.81 to 8.08. The most prominent alteration was found in Cough syrup-Alkasite(8.08 ± 2.62) and the least one was found in Cough syrup-HVGIC(1.81 ± 0.74) pairwise. The color change observed in Cough syrup-Alkasite group was statistically significantly higher than in Cough syrup-HVGIC (p < 0.05). Alkasite showed greater color alteration with all drugs compared to other materials and HVGIC showed better color stability with all drug formulations.
引用
收藏
页码:601 / 608
页数:7
相关论文
共 131 条
[1]  
Faghihi T(2021)An experimental study on the effect of four pediatric drug types on color stability in different tooth-colored restorative materials Dent Res J 18 75-603
[2]  
Heidarzadeh Z(2020)Evaluation of extrinsic discoloration of new alkasite resin with the microhybrid composite using natural beverages: An in vitro study Intl J Appl Dent Sci 6 600-29
[3]  
Jafari K(2022)In vivo evaluation of clinical performance of Cention N and glass ionomer cement in proximal restorations of primary molars J. Indian Soc. Pedod. Prev. Dent. 40 23-107
[4]  
Farhoudi I(2022)Evaluation of Alkalizing Potential of Alkasite Restorations Prepared in Different Sizes Cumhuriyet Dent. J. 25 100-1877
[5]  
Hekmatfar S(2022)Ion releasing direct restorative materials: Key mechanical properties and wear Dent. Mater. 38 1866-673
[6]  
Chakravarthy Y(2021)Comparative evaluation of mechanical and physical properties of a new bulk-fill alkasite with conventional restorative materials Saudi. Dent. J. 33 666-618
[7]  
Raja Nanthini AC(2020)Effects of different pediatric drugs and toothbrushing on color change of restorative materials used in pediatric dentistry Niger. J. Clin. Pract. 23 610-156
[8]  
Arora D(2019)Effect of different pediatric drug formulations on color stability of composite, zirconia-reinforced glass ionomer cement, and glass ionomer cement J. Indian Soc. Pedod. Prev. Dent. 37 151-13
[9]  
Jain M(2023)Color stability evaluation of different posterior composites Essent Dent 2 9-407
[10]  
Sogi HP(2019)Comparative evaluation of microleakage around Class V cavities restored with alkasite restorative material with and without bonding agent and flowable composite resin: An in vitro study Indian. J. Dent. Res. 30 403-695