Influence of grain refinement on hot cracking in laser welding of aluminum

被引:0
|
作者
Zhuo Tang
Frank Vollertsen
机构
[1] Bremer Institut fuer Angewandte Strahltechnik GmbH (BIAS),
来源
Welding in the World | 2014年 / 58卷
关键词
Hot cracking; Grain refinement; Aluminum; Laser welding; Modeling;
D O I
暂无
中图分类号
学科分类号
摘要
Hot cracking is a major problem in casting and laser welding of important technical aluminum alloys. A well-known method to reduce this problem is grain refinement. The mechanism of hot cracking prevention by grain refinement is not fully understood yet. In this study, different amounts of titanium and boron were added into weld in laser welding of AA 6082, which lead to different grain structures. A hot cracking test (DELTA test) was carried out to investigate the influence of grain refinement on hot cracking susceptibility of the welds. In order to understand the mechanism of hot cracking prevention by grain refinement, an analytical model was developed, which describes the influences of the grain structure and solidifications parameter on the three following factors, the duration of the mush zone, the capillary pressure for hot cracking, as well as the permeability of the dendritic network in the molten pool. It reveals that the hot cracking susceptibility is determined by the combination effect of these three factors. There is an optimum grain size for a minimal hot cracking susceptibility. It agrees with the experimental results in DELTA test.
引用
收藏
页码:355 / 366
页数:11
相关论文
共 50 条
  • [11] Influence of grain refinement on hot tearing in B206 and A319 aluminum alloys
    D'Elia, F.
    Ravindran, C.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2009, 62 (4-5) : 315 - 319
  • [12] Influence of grain refinement on hot tearing in B206 and A319 aluminum alloys
    F. D’Elia
    C. Ravindran
    Transactions of the Indian Institute of Metals, 2009, 62 : 315 - 319
  • [13] Effect of TiN Spray Coating on Cracking Susceptibility and Energy Absorption in Laser Welding of Aluminum Alloys
    Nam, Sangwoo
    Jung, In-Ho
    Kim, Young-Min
    METALS, 2020, 10 (12) : 1 - 10
  • [14] Hot cracking in pulsed Nd:YAG laser welding of AA5456
    Hekmatjou, Hamidreza
    Naffakh-Moosavy, Homam
    OPTICS AND LASER TECHNOLOGY, 2018, 103 : 22 - 32
  • [15] Reduction of hot cracking in laser welding using hypereutectic AlSi filler wire
    Vollertsen F.
    Buschenhenke F.
    Seefeld T.
    Welding in the World, 2008, 52 (5-6) : 3 - 8
  • [16] Investigation on hot cracking during laser welding by means of experimental and numerical methods
    Gao, H.
    Agarwal, G.
    Amirthalingam, M.
    Hermans, M. J. M.
    Richardson, I. M.
    WELDING IN THE WORLD, 2018, 62 (01) : 71 - 78
  • [17] Investigation on hot cracking during laser welding by means of experimental and numerical methods
    H. Gao
    G. Agarwal
    M. Amirthalingam
    M. J. M. Hermans
    I. M. Richardson
    Welding in the World, 2018, 62 : 71 - 78
  • [18] Effect of Preheating on Hot Cracking Susceptibility in Pulsed Laser Welding of Invar Alloy
    Zhao, DongSheng
    Wu, Liangliang
    Zhang, TianFei
    Kong, Lele
    Liu, YuJun
    JOURNAL OF SHIP PRODUCTION AND DESIGN, 2022, 38 (01): : 19 - 27
  • [19] Effects of grain refinement and residual elements on hot tearing in aluminum castings
    Karunakar, D. Benny
    Rai, Ram Naresh
    Patra, Suprakash
    Datta, G. L.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2009, 45 (9-10) : 851 - 858
  • [20] Effects of grain refinement and residual elements on hot tearing in aluminum castings
    D. Benny Karunakar
    Ram Naresh Rai
    Suprakash Patra
    G. L. Datta
    The International Journal of Advanced Manufacturing Technology, 2009, 45 : 851 - 858