Hot Corrosion Behavior of Si–Y–Co-Modified Aluminide Coating Exposed to NaCl + Na2SO4 Salt at 1173 K

被引:1
|
作者
Zongjie Liu
Chungen Zhou
机构
[1] Beijing University of Aeronautics and Astronautics,Key Laboratory of Aerospace Materials and Performance (Ministry of Education), School of Materials Science and Engineering
来源
Oxidation of Metals | 2016年 / 85卷
关键词
Metal coatings; Superalloys; Hot corrosion;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:205 / 217
页数:12
相关论文
共 50 条
  • [31] Hot corrosion behavior and mechanism of FGH96 P/M superalloy in molten NaCl–Na2SO4 salts
    He Jiang
    Jian-Xin Dong
    Mai-Cang Zhang
    Lei Zheng
    Zhi-Hao Yao
    Rare Metals, 2019, 38 (02) : 173 - 180
  • [32] Hot corrosion behaviour of Nbss/Nb5Si3 in situ composites in the mixture of Na2SO4 and NaCl melts
    Wang, Wan
    Zhou, Chungen
    CORROSION SCIENCE, 2013, 74 : 345 - 352
  • [33] Effects of Pt and Si on the low temperature hot corrosion of aluminide coatings exposed to Na2SO4-60 mol% V2O5 salt
    Azarmehr, S. A.
    Shirvani, K.
    Solimani, A.
    Schuetze, M.
    Galetz, M. C.
    SURFACE & COATINGS TECHNOLOGY, 2019, 362 : 252 - 261
  • [34] Hot corrosion behavior of Mg2SiO4 ceramic exposed to molten Na2SO4 at 900°C to 1100°C
    Milles, Hamza
    Snani, Louafi
    Oulabbas, Amel
    Toualbia, Khaled
    JOURNAL OF METALS MATERIALS AND MINERALS, 2024, 34 (01):
  • [35] Hot corrosion behavior of AlCoCrFeNiZr high entropy alloy (HEA) coating system exposed to Na2SO4-V2O5 salt
    Odabas, Okan
    Ozgurluk, Yasin
    Karaoglanli, Abdullah Cahit
    MATERIALS TODAY COMMUNICATIONS, 2025, 45
  • [36] Effect of Minor Nb on Isothermal-Oxidation and Hot Corrosion Behavior of Two Nickel-Based Superalloys Under Na2SO4/Na2SO4-NaCl
    Zhou, Yuebo
    Wang, Hong
    Mo, Chenggang
    Zhang, Lina
    CORROSION, 2021, 77 (09) : 949 - 960
  • [37] Crevice Formation on the Surface of the Simple and Ti-Modified Aluminide Coatings Under a Fused Na2SO4 Salt Film
    Shahriari, Farhad
    Saatchi, Ahmad
    Ashrafizadeh, Fakhreddin
    OXIDATION OF METALS, 2011, 76 (1-2): : 57 - 65
  • [38] Hot corrosion behaviour of Inconel 738 superalloy in presence of NaCl, Na2SO4, V2O5
    Patil, Arpit R.
    Vagge, S. T.
    MATERIALS TODAY-PROCEEDINGS, 2022, 65 : 74 - 80
  • [39] Crevice Formation on the Surface of the Simple and Ti-Modified Aluminide Coatings Under a Fused Na2SO4 Salt Film
    Farhad Shahriari
    Ahmad Saatchi
    Fakhreddin Ashrafizadeh
    Oxidation of Metals, 2011, 76 : 57 - 65
  • [40] Electrochemical study on hot corrosion of Si-modified aluminide coated In-738LC in Na2SO4-20 wt.% NaCl melt at 750°C
    Shirvani, K
    Saremi, M
    Nishikata, A
    Tsuru, T
    CORROSION SCIENCE, 2003, 45 (05) : 1011 - 1021