Resistance of a Mo–Si–B-Based Coating to Environmental Salt-Based Hot Corrosion

被引:0
作者
Eric Auchter
Matthew Taylor
John H. Perepezko
机构
[1] University of Wisconsin-Madison,Department of Materials Science and Engineering
来源
Oxidation of Metals | 2020年 / 93卷
关键词
Hot corrosion; Magnesium sulfate; Mo–Si–B; Coating; High-temperature materials;
D O I
暂无
中图分类号
学科分类号
摘要
During operation of gas turbine engines, different salts develop that lead to a hot-corrosion attack. While the hot corrosion associated with Na2SO4 and Na3VO4 has received considerable attention, MgSO4 is also a main salt component, but it has received limited examination. For operation at temperatures beyond the capabilities of Ni-base superalloys, refractory-metal alloys with a Mo–Si–B-based coating have demonstrated a robust environmental resistance including hot corrosion attack by Na2SO4 and Na3VO4. In order to evaluate the performance of Mo with a Mo–Si–B-based amorphous coating, samples were exposed to MgSO4 under thermal cycling at temperatures from 800 to 1300 °C. Mass change measurements revealed minimal attack from the MgSO4 exposure except in local regions where cristobalite and MgMoO4 were detected. Even with the local region reaction, the mass change after a cumulative 100 h of exposure was about 3.5 mg/cm2. Exposure to a composite salt mixture containing Na2SO4, NaVO3, MgSO4, CaCl, and KCl revealed signs of interactivity compared to the corrosion due to the separate effects of the individual salts, but again the mass change stabilized to a minimal level demonstrating that the Mo–Si–B-based coating is resilient to hot corrosion.
引用
收藏
页码:387 / 399
页数:12
相关论文
共 50 条
  • [31] Hot corrosion phenomena of Nb-Ti-Si based alloy and its silicide coating induced by different corrosive environments at 900 °C
    Qiao, Yanqiang
    Kong, Jianping
    Guo, Xiping
    CERAMICS INTERNATIONAL, 2018, 44 (07) : 7978 - 7990
  • [32] Oxidation and Hot Corrosion Resistance of HVOF WC-NiCrFeSiB Coating on Ni- and Fe-based Superalloys at 800 °C
    T. S. Sidhu
    A. Malik
    S. Prakash
    R. D. Agrawal
    Journal of Thermal Spray Technology, 2007, 16 : 844 - 849
  • [33] Influence of NiCoCrAlY and diffusion aluminide coating on oxidation and hot corrosion of a Ni-based superalloy
    Xie, Dongbai
    Zhu, Shenglong
    Dai, Wenjun
    Wang, Fuhui
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1739 - +
  • [34] Hot Corrosion Behavior of a Cr-Modified Aluminide Coating on a Ni-Based Superalloy
    Duoli Wu
    Sumeng Jiang
    Qixiang Fan
    Jun Gong
    Chao Sun
    ActaMetallurgicaSinica(EnglishLetters), 2014, 27 (04) : 627 - 634
  • [35] Hot Corrosion Behavior of a Cr-Modified Aluminide Coating on a Ni-Based Superalloy
    Wu, Duoli
    Jiang, Sumeng
    Fan, Qixiang
    Gong, Jun
    Sun, Chao
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2014, 27 (04) : 627 - 634
  • [36] Hot Corrosion Behavior of a Cr-Modified Aluminide Coating on a Ni-Based Superalloy
    Duoli Wu
    Sumeng Jiang
    Qixiang Fan
    Jun Gong
    Chao Sun
    Acta Metallurgica Sinica (English Letters), 2014, 27 : 627 - 634
  • [37] Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy
    Liu, R. D.
    Jiang, S. M.
    Yu, H. J.
    Gong, J.
    Sun, C.
    CORROSION SCIENCE, 2016, 104 : 162 - 172
  • [38] Effects of structural relaxation and crystallization on the corrosion resistance of an Fe-based amorphous coating
    Kang, Yonghai
    Chen, Youming
    Wen, Yuxin
    Wu, Bo
    Song, Mengbin
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2020, 550
  • [39] STUDY ON HOT CORROSION RESISTANCE OF A NEW DIRECTIONAL SOLIDIFICATION Ni-BASED SUPERALLOY
    Ning Likui
    Zheng Zhi
    Tan Yi
    Liu Enze
    Tong Jian
    Yu Yongsi
    Wang Hua
    ACTA METALLURGICA SINICA, 2009, 45 (02) : 161 - 166
  • [40] Wear resistance and hot corrosion behaviour of laser cladding Co-based alloy
    Zhang, S
    Zhang, CH
    Man, HC
    Wu, WT
    Wang, MC