Fracture properties of high-strength/high-performance concrete (HSC/HPC) exposed to high temperature

被引:0
作者
Kequan Yu
Jiangtao Yu
Zhoudao Lu
Qingyang Chen
机构
[1] Tongji University,College of Civil Engineering
来源
Materials and Structures | 2016年 / 49卷
关键词
High temperature; High-strength/high-performance concrete; Fracture properties; Digital image correlation;
D O I
暂无
中图分类号
学科分类号
摘要
An investigation of the residual fracture properties of high-strength/high-performance concrete (C80 and C100) exposed to high temperatures is reported in this article. Three-point bending test specimens of 100 mm × 100 mm × 515 mm size were prepared according to the RILEM recommendation. The three-point bending beams were exposed to temperatures varying from 200 to 800 °C. The complete load-crack mouth opening displacement curves and load-deflection curves of the specimen were worked out after cooling. The fracture toughness, including the initial and unstable fracture toughness, fracture energy, and characteristic length, was calculated. These four parameters were shown to decrease monotonically with temperature. Other mechanical properties including the compressive strength, compressive Young’s modulus, and splitting strength of post-fire specimens were also obtained. The digital image correlation method was utilized to monitor the whole fracture process, and the results from the digital image correlation method fit well with those from the direct measurements.
引用
收藏
页码:4517 / 4532
页数:15
相关论文
共 83 条
[1]  
Baker G(1996)The effect of exposure to elevated temperatures on the fracture energy of plain concrete RILEM Mater Struct 29 383-388
[2]  
Bamonte P(2009)Thermal and mechanical properties at high temperature of a very high-strength durable concrete J Mater Civ Eng 22 545-555
[3]  
Gambarova PG(2012)A study on the mechanical properties of self-compacting concrete at high temperature and after cooling Mater Struct 45 1375-1387
[4]  
Bamonte P(1988)Effect of temperatures and humidity on fracture energy of concrete ACI Mater J 85 262-271
[5]  
Gambarova PG(2009)Comparison of compressive and splitting tensile strength of high-strength/high-performance concrete with and without polypropylene fibers heated to high temperatures Fire Saf J 44 1015-1022
[6]  
Bazant ZP(2008)Evaluating residual properties of thermally damaged concrete Cement Concr Compos 30 907-916
[7]  
Prat PC(1990)Effect of transient high temperature on high strength concrete ACI Mater J 86 47-53
[8]  
Behnood A(1999)Residual strength and pore structure of high-strength/high-performance concrete and normal strength concrete after exposure to high temperatures Cement Concr Compos 21 23-27
[9]  
Ghandehari M(1999)Fire behavior of high-performance concrete made with silica fume at various moisture contents ACI Mater J 96 405-409
[10]  
Biolzi L(2000)Compressive strength and pore structure of high-performance concrete after exposure to high temperature up to 800 °C Cem Concr Res 30 247-251