On the Influence of Strain Rate and Number of Passes on Grain Refinement in Al-Mg-Si Alloy Processed by Cyclic Expansion Extrusion

被引:0
作者
V. Babu
Balasivanandha Prabu Shanmugavel
K. A. Padmanabhan
机构
[1] Anna University,Department of Mechanical Engineering, College of Engineering Guindy
来源
Journal of Materials Engineering and Performance | 2020年 / 29卷
关键词
cyclic expansion extrusion; grain refinement; mechanical properties; severe plastic deformation;
D O I
暂无
中图分类号
学科分类号
摘要
The effects of the strain rate (3.1 × 10−2 s−1, 1.5 × 10−2 s−1 and 7.7 × 10−3 s−1) and the number of passes on grain refinement in an Al-Mg-Si alloy (AA 6063) processed by cyclic expansion extrusion (CEE) at 150 °C are discussed. Specimens processed up to 8 passes at a strain rate of 7.7 × 10−3 s−1 displayed an increased micro-hardness value of 114 HV and tensile strength of 195 MPa, which represent 200 and 65% increase, respectively, on the properties of the parent material. The electron backscatter diffraction images revealed that the slowest strain rate grain refinement was maximal on reaching an average grain size of 3 µm after 8 passes. The grain size distribution in the material after the CEE process was uniform, and a majority of grain boundaries were of the low-angle type. The TEM analysis also confirmed that after 8 passes, the grain refinement was maximum at a strain rate of 7.7 × 10−3 s−1. A reduction in the degree of dynamic recrystallization with an increasing strain rate (3.1 × 10−2 s−1 and 1.5 × 10−2 s−1) decreases the extent of fine grain formation. As a result, the strength properties were inferior at the higher strain rates due to the well-known Hall–Petch (H–P) effect, i.e., grain refinement decreases at the higher strain rates. In fact, the H–P relation is obeyed in the material processed at all the three different strain rates. Another feature is that in the CEE processed material, the H–P slope (ky) was less steep and the intercept value (σo) greater as the strain rate decreased.
引用
收藏
页码:8049 / 8059
页数:10
相关论文
共 180 条
[31]  
Orlov D(2019)Microstructure and Mechanical Properties of AA6061-5wt.% TiB Mater. Sci. Eng. A 26 5488-16
[32]  
Beygelzimer Y(2001) In Situ Metal Matrix Composite Subjected to Equal Channel Angular Pressing Philos. Mag. A 197 12-4317
[33]  
Synkov S(1991)Grain Refinement in Copper Under Large Strain Deformation J. Mater. Sci. 528 4312-4779
[34]  
Varyukhin V(2017)Axi-Symmetric Compression of Solid Cylinders Mater. Lett. 56 4771-60
[35]  
Suji TN(2011)Cyclic Extrusion Compression Angular Pressing (CECAP) as a Novel Severe Plastic Deformation Method for Producing Bulk Ultrafine Grained Metals Mater. Sci. Eng. A 527 52-116
[36]  
Horita Z(2008)Microstructure Inhomogeneity in Ultra-Fine Grained Bulk AZ91 Produced by Accumulative Back Extrusion (ABE) Acta Mater. 483 113-563
[37]  
Lianxi H(2009)A New Constitutive Equation for Strain Hardening and Softening of FCC Metals during Severe Plastic Deformation Mater. Sci. Eng. A 63 560-574
[38]  
Yuping L(2008)Recrystallization Mechanism of As-Cast AZ91 Magnesium Alloy During Hot Compressive Deformation Mater. Sci. Eng. A 111 548-48
[39]  
Erde W(2010)Equal-Channel Angular Pressing of Magnesium Alloy AZ91 and Its Effects on Microstructure and Mechanical Properties Scr. Mater. 58 41-1875
[40]  
Yang Y(2016)Evolution of Microstructural Homogeneity in Copper Processed by High-Pressure Torsion Mater. Des. 29 1865-248