Hot Corrosion of a Single Crystal Ni-Base Superalloy by Na-Salts at 900°C

被引:18
作者
Meiheng Li
Xiaofeng Sun
Wangyu Hu
Hengrong Guan
Shuguang Chen
机构
[1] Hunan University,Department of Applied Physics
[2] Chinese Academy of Sciences,Institute of Metal Research
来源
Oxidation of Metals | 2006年 / 65卷
关键词
single crystal Ni-base superalloy; hot corrosion; molten salt; microstructure;
D O I
暂无
中图分类号
学科分类号
摘要
The hot corrosion behaviors of a single crystal (SC) Ni-base superalloy coated with Na2SO4 and 75 wt.% Na2SO4-25 wt.% NaCl mixture were studied in air at 900°C. The results showed that the corrosion productions were laminar structure, porous and easily spalled. And sulfides formed quickly in the deep SC superalloy under the corrosion production. The addition of NaCl into Na2SO4 considerably accelerated the corrosion of the SC superalloy, and the corrosion scale became more porous. The hot corrosion process was explained based on sulfide formation and its subsequent oxidation.
引用
收藏
页码:137 / 150
页数:13
相关论文
共 64 条
  • [1] Li M.H.(2004)undefined Surface Coatings Technology 176 209-undefined
  • [2] Sun X.F.(2002)undefined Oxidation of Metals 58 499-undefined
  • [3] Gong S.K.(2003)undefined Surface Coatings Technology 163–164 95-undefined
  • [4] Zhang Z.Y.(2003)undefined Surface Coatings Technology 165 241-undefined
  • [5] Guan H.R.(2003)undefined Surface Coating Technology 163 81-undefined
  • [6] Hu Z.Q.(2003)undefined Oxidation of Metals 59 591-undefined
  • [7] Li M.H.(2003)undefined Oxidation of Metals 60 195-undefined
  • [8] Zhang Z.Y.(1996)undefined Materials Letters 29 19-undefined
  • [9] Sun X.F.(1969)undefined Transactions of the Metallurgical society of AIME 245 1947-undefined
  • [10] Guan H.R.(1978)undefined Metallurgical Transactions A9 1055-undefined